Failure Study of BFRP Joints with Two Epoxy Adhesives under Hygrothermal Coupling
Basalt Fibre Reinforced Polymer (BFRP)-bonded structures are lightweight, high strength, economical, and environmentally friendly, which is very advantageous in the civil sector. The aim of this paper is to provide a comprehensive account of the hygrothermal degradation and failure mechanisms of BFR...
Autores principales: | , , , , |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
MDPI
2023
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC10574937/ https://www.ncbi.nlm.nih.gov/pubmed/37835997 http://dx.doi.org/10.3390/polym15193949 |
_version_ | 1785120805934333952 |
---|---|
author | Niu, Ruitao Yang, Yang Lin, Yinghao Liu, Zhen Fan, Yisa |
author_facet | Niu, Ruitao Yang, Yang Lin, Yinghao Liu, Zhen Fan, Yisa |
author_sort | Niu, Ruitao |
collection | PubMed |
description | Basalt Fibre Reinforced Polymer (BFRP)-bonded structures are lightweight, high strength, economical, and environmentally friendly, which is very advantageous in the civil sector. The aim of this paper is to provide a comprehensive account of the hygrothermal degradation and failure mechanisms of BFRP-bonded structures by comparing the residual properties of two epoxy adhesive BFRP single-lap joints after ageing for 240 h, 480 h, and 720 h in an extreme hygrothermal environment with pure water at 80 °C. The hydrophilicity and thermal stability of the two adhesives were firstly compared by water absorption and Thermogravimetric Analysis (TGA) tests, and the hygrothermal degradation of the molecular chains and the reduction in T(g) were characterised by Fourier Transform Infra-Red (FTIR) spectroscopy and Differential Scanning Calorimetry (DSC) curves. The failure strength and load-displacement curves of the two joints were then compared, and it was found that the strength and stiffness had different trends, while the paired t-test was used to demonstrate the correlation between the failure strength and the adhesive T(g), as well as the difference in the failure mechanisms of the two joints caused by the water absorption rate. The analysis of macrosections and Scanning Electron Microscope (SEM) images summarised the process and reasons for the transition of the failure mode from fibre tearing to hybrid failure, and finally, the changes in elemental concentration and O/C values were analysed by Energy Dispersive X-ray Analysis (EDX), which proved that the degree of hydrolysis could not be used as a judgement of the degradation degree of the joint alone, and provided data support for the application of the BFRP-bonded structure in the humid and hot environment. |
format | Online Article Text |
id | pubmed-10574937 |
institution | National Center for Biotechnology Information |
language | English |
publishDate | 2023 |
publisher | MDPI |
record_format | MEDLINE/PubMed |
spelling | pubmed-105749372023-10-14 Failure Study of BFRP Joints with Two Epoxy Adhesives under Hygrothermal Coupling Niu, Ruitao Yang, Yang Lin, Yinghao Liu, Zhen Fan, Yisa Polymers (Basel) Article Basalt Fibre Reinforced Polymer (BFRP)-bonded structures are lightweight, high strength, economical, and environmentally friendly, which is very advantageous in the civil sector. The aim of this paper is to provide a comprehensive account of the hygrothermal degradation and failure mechanisms of BFRP-bonded structures by comparing the residual properties of two epoxy adhesive BFRP single-lap joints after ageing for 240 h, 480 h, and 720 h in an extreme hygrothermal environment with pure water at 80 °C. The hydrophilicity and thermal stability of the two adhesives were firstly compared by water absorption and Thermogravimetric Analysis (TGA) tests, and the hygrothermal degradation of the molecular chains and the reduction in T(g) were characterised by Fourier Transform Infra-Red (FTIR) spectroscopy and Differential Scanning Calorimetry (DSC) curves. The failure strength and load-displacement curves of the two joints were then compared, and it was found that the strength and stiffness had different trends, while the paired t-test was used to demonstrate the correlation between the failure strength and the adhesive T(g), as well as the difference in the failure mechanisms of the two joints caused by the water absorption rate. The analysis of macrosections and Scanning Electron Microscope (SEM) images summarised the process and reasons for the transition of the failure mode from fibre tearing to hybrid failure, and finally, the changes in elemental concentration and O/C values were analysed by Energy Dispersive X-ray Analysis (EDX), which proved that the degree of hydrolysis could not be used as a judgement of the degradation degree of the joint alone, and provided data support for the application of the BFRP-bonded structure in the humid and hot environment. MDPI 2023-09-29 /pmc/articles/PMC10574937/ /pubmed/37835997 http://dx.doi.org/10.3390/polym15193949 Text en © 2023 by the authors. https://creativecommons.org/licenses/by/4.0/Licensee MDPI, Basel, Switzerland. This article is an open access article distributed under the terms and conditions of the Creative Commons Attribution (CC BY) license (https://creativecommons.org/licenses/by/4.0/). |
spellingShingle | Article Niu, Ruitao Yang, Yang Lin, Yinghao Liu, Zhen Fan, Yisa Failure Study of BFRP Joints with Two Epoxy Adhesives under Hygrothermal Coupling |
title | Failure Study of BFRP Joints with Two Epoxy Adhesives under Hygrothermal Coupling |
title_full | Failure Study of BFRP Joints with Two Epoxy Adhesives under Hygrothermal Coupling |
title_fullStr | Failure Study of BFRP Joints with Two Epoxy Adhesives under Hygrothermal Coupling |
title_full_unstemmed | Failure Study of BFRP Joints with Two Epoxy Adhesives under Hygrothermal Coupling |
title_short | Failure Study of BFRP Joints with Two Epoxy Adhesives under Hygrothermal Coupling |
title_sort | failure study of bfrp joints with two epoxy adhesives under hygrothermal coupling |
topic | Article |
url | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC10574937/ https://www.ncbi.nlm.nih.gov/pubmed/37835997 http://dx.doi.org/10.3390/polym15193949 |
work_keys_str_mv | AT niuruitao failurestudyofbfrpjointswithtwoepoxyadhesivesunderhygrothermalcoupling AT yangyang failurestudyofbfrpjointswithtwoepoxyadhesivesunderhygrothermalcoupling AT linyinghao failurestudyofbfrpjointswithtwoepoxyadhesivesunderhygrothermalcoupling AT liuzhen failurestudyofbfrpjointswithtwoepoxyadhesivesunderhygrothermalcoupling AT fanyisa failurestudyofbfrpjointswithtwoepoxyadhesivesunderhygrothermalcoupling |