Cargando…
Experimental Investigation on Pore-Fracture Variations in Coal Affected by Carbon Disulfide
[Image: see text] Solvent treatment is an effective technique to stimulate pore and fracture growth in low-permeability coal seams and improve the efficiency of methane extraction. Adopting the nuclear magnetic resonance test, liquid nitrogen adsorption analysis, ultrasonic test, and CT scanning, po...
Autores principales: | , , , , |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
American Chemical Society
2023
|
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC10586306/ https://www.ncbi.nlm.nih.gov/pubmed/37867664 http://dx.doi.org/10.1021/acsomega.3c05203 |
_version_ | 1785123131317288960 |
---|---|
author | Zheng, Chunshan Li, Xing Li, He Jiang, Bingyou Chen, Zhongwei |
author_facet | Zheng, Chunshan Li, Xing Li, He Jiang, Bingyou Chen, Zhongwei |
author_sort | Zheng, Chunshan |
collection | PubMed |
description | [Image: see text] Solvent treatment is an effective technique to stimulate pore and fracture growth in low-permeability coal seams and improve the efficiency of methane extraction. Adopting the nuclear magnetic resonance test, liquid nitrogen adsorption analysis, ultrasonic test, and CT scanning, pore variation and fracture development in lignite, bituminous coal, and anthracite after carbon disulfide treatment were analyzed. Full-scale pore size distribution characteristics were obtained. The Frenkel–Halsey–Hill model was adopted to analyze pore fractal properties. Experiment results show that carbon disulfide could increase coal porosity. Lignite showed the best pore alteration effect, with a porosity increase of 34.10%, followed by bituminous coal with a porosity increase of 14.55%, while anthracite had a slightly weaker change with only 0.91% porosity growth. The pore diameter distribution range of treated coal expanded from 0–450 to 0–1000 μm. The average pore diameter rose from 316 to 483 μm, with better connectivity between pores. After treatment, the proportions of micropore specific surface areas (SSA) in three coal samples decreased but the ratios of small pore and medium pore SSA increased. Fractal dimension D(1) of lignite and bituminous coal decreased by 5.669 and 0.054%, while D(1) of anthracite increased by 22.407%. D(2) reduced by 0.599, 3.143, and 1.262%, respectively. Raw coal had the maximum porosity near both ends of the CT section. Porosity of lignite was the largest at the ends after treatment. Surface porosity inside coal samples also rose from about 0.1 in raw coal to approximately 0.4 after treatment. Ultrasonic velocity in lignite decreased by 50.16% due to solvent treatment. Increases in ultrasonic attenuation coefficient α and ultrasonic attenuation ratio β indicate good fracture development. Furthermore, development degrees of lignite and bituminous coal are higher than that of anthracite. Results of the above methods verify with each other, indicating the effectiveness of carbon disulfide treatment in improving pore and fracture structures. The outcomes of this research could offer a theoretical basis for chemical permeability-enhancement technology. |
format | Online Article Text |
id | pubmed-10586306 |
institution | National Center for Biotechnology Information |
language | English |
publishDate | 2023 |
publisher | American Chemical Society |
record_format | MEDLINE/PubMed |
spelling | pubmed-105863062023-10-20 Experimental Investigation on Pore-Fracture Variations in Coal Affected by Carbon Disulfide Zheng, Chunshan Li, Xing Li, He Jiang, Bingyou Chen, Zhongwei ACS Omega [Image: see text] Solvent treatment is an effective technique to stimulate pore and fracture growth in low-permeability coal seams and improve the efficiency of methane extraction. Adopting the nuclear magnetic resonance test, liquid nitrogen adsorption analysis, ultrasonic test, and CT scanning, pore variation and fracture development in lignite, bituminous coal, and anthracite after carbon disulfide treatment were analyzed. Full-scale pore size distribution characteristics were obtained. The Frenkel–Halsey–Hill model was adopted to analyze pore fractal properties. Experiment results show that carbon disulfide could increase coal porosity. Lignite showed the best pore alteration effect, with a porosity increase of 34.10%, followed by bituminous coal with a porosity increase of 14.55%, while anthracite had a slightly weaker change with only 0.91% porosity growth. The pore diameter distribution range of treated coal expanded from 0–450 to 0–1000 μm. The average pore diameter rose from 316 to 483 μm, with better connectivity between pores. After treatment, the proportions of micropore specific surface areas (SSA) in three coal samples decreased but the ratios of small pore and medium pore SSA increased. Fractal dimension D(1) of lignite and bituminous coal decreased by 5.669 and 0.054%, while D(1) of anthracite increased by 22.407%. D(2) reduced by 0.599, 3.143, and 1.262%, respectively. Raw coal had the maximum porosity near both ends of the CT section. Porosity of lignite was the largest at the ends after treatment. Surface porosity inside coal samples also rose from about 0.1 in raw coal to approximately 0.4 after treatment. Ultrasonic velocity in lignite decreased by 50.16% due to solvent treatment. Increases in ultrasonic attenuation coefficient α and ultrasonic attenuation ratio β indicate good fracture development. Furthermore, development degrees of lignite and bituminous coal are higher than that of anthracite. Results of the above methods verify with each other, indicating the effectiveness of carbon disulfide treatment in improving pore and fracture structures. The outcomes of this research could offer a theoretical basis for chemical permeability-enhancement technology. American Chemical Society 2023-10-03 /pmc/articles/PMC10586306/ /pubmed/37867664 http://dx.doi.org/10.1021/acsomega.3c05203 Text en © 2023 The Authors. Published by American Chemical Society https://creativecommons.org/licenses/by-nc-nd/4.0/Permits non-commercial access and re-use, provided that author attribution and integrity are maintained; but does not permit creation of adaptations or other derivative works (https://creativecommons.org/licenses/by-nc-nd/4.0/). |
spellingShingle | Zheng, Chunshan Li, Xing Li, He Jiang, Bingyou Chen, Zhongwei Experimental Investigation on Pore-Fracture Variations in Coal Affected by Carbon Disulfide |
title | Experimental Investigation on Pore-Fracture Variations
in Coal Affected by Carbon Disulfide |
title_full | Experimental Investigation on Pore-Fracture Variations
in Coal Affected by Carbon Disulfide |
title_fullStr | Experimental Investigation on Pore-Fracture Variations
in Coal Affected by Carbon Disulfide |
title_full_unstemmed | Experimental Investigation on Pore-Fracture Variations
in Coal Affected by Carbon Disulfide |
title_short | Experimental Investigation on Pore-Fracture Variations
in Coal Affected by Carbon Disulfide |
title_sort | experimental investigation on pore-fracture variations
in coal affected by carbon disulfide |
url | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC10586306/ https://www.ncbi.nlm.nih.gov/pubmed/37867664 http://dx.doi.org/10.1021/acsomega.3c05203 |
work_keys_str_mv | AT zhengchunshan experimentalinvestigationonporefracturevariationsincoalaffectedbycarbondisulfide AT lixing experimentalinvestigationonporefracturevariationsincoalaffectedbycarbondisulfide AT lihe experimentalinvestigationonporefracturevariationsincoalaffectedbycarbondisulfide AT jiangbingyou experimentalinvestigationonporefracturevariationsincoalaffectedbycarbondisulfide AT chenzhongwei experimentalinvestigationonporefracturevariationsincoalaffectedbycarbondisulfide |