Thermo-Mechanical Treatment for Reducing the Wear Rate of CuCrZr Tool Electrodes during Electro-Discharge Machining

The research presented in this paper focused on optimising the process of unconventional plastic forming by hydrostatic extrusion (HE) with post-processing heat treatment of a copper alloy (CuCrZr) for electro-discharge machining (EDM) applications. The treatment was carried out in such a way as to...

Descripción completa

Detalles Bibliográficos
Autores principales: Skiba, Jacek, Kulczyk, Mariusz, Przybysz-Gloc, Sylwia, Skorupska, Monika, Smalc-Koziorowska, Julita, Kobus, Mariusz, Nowak, Kamil
Formato: Online Artículo Texto
Lenguaje:English
Publicado: MDPI 2023
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC10608494/
https://www.ncbi.nlm.nih.gov/pubmed/37895768
http://dx.doi.org/10.3390/ma16206787
Descripción
Sumario:The research presented in this paper focused on optimising the process of unconventional plastic forming by hydrostatic extrusion (HE) with post-processing heat treatment of a copper alloy (CuCrZr) for electro-discharge machining (EDM) applications. The treatment was carried out in such a way as to obtain a material with an improved microstructure, characterised by a significant increase in hardness and strength while maintaining a high electrical conductivity, thus achieving the main goal of reducing electrode wear in the EDM process. As part of the research, a material with an ultrafine-grained structure was obtained with an average grain size of d(2) = 320 nm and a much higher strength of UTS = 645 MPa compared to the material in the initial state (UTS = 413 MPa). The post-processing treatment (ageing) allowed us to obtain a material with a high electrical conductivity after the HE process, at 78% IACS. The electrodes made of CuCrZr subjected to HE had a reduced electrical discharge wear in relation to electrodes made of the initial material. The best results were obtained for electrodes made of the material subjected to a five-stage HE process combined with ageing at 480 °C for 1 h. The electrical discharge wear in these electrodes was reduced by more than 50% compared to electrodes made of non-deformed copper.