Cargando…
Femtosecond Laser Machining of an X-ray Mask in a 500 Micron-Thick Tungsten Sheet
Femtosecond laser material processing (FLMP) was used to make an X-ray mask in a 500 µm thick tungsten sheet without the use of any chemical etch methods. The laser produced an 800 nm wavelength at a 1 kHz repetition rate and a pulse width of 100 fs. The laser beam arrival at the tungsten sheet was...
Autores principales: | Owusu-Ansah, Ebenezer, Dalton, Colin |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
MDPI
2023
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC10673140/ https://www.ncbi.nlm.nih.gov/pubmed/38004928 http://dx.doi.org/10.3390/mi14112071 |
Ejemplares similares
-
Fabrication of a 3D Multi-Depth Reservoir Micromodel in Borosilicate Glass Using Femtosecond Laser Material Processing
por: Owusu-Ansah, Ebenezer, et al.
Publicado: (2020) -
AFM Analysis of Micron and Sub-Micron Sized Bridges Fabricated Using the Femtosecond Laser on YBCO Thin Films
por: Umenne, Patrice
Publicado: (2020) -
Femtosecond Laser
Micromachining of the Mask for Acoustofluidic
Device Preparation
por: Wang, Yong, et al.
Publicado: (2023) -
Formation of Subwavelength Periodic Triangular Arrays on Tungsten through Double-Pulsed Femtosecond Laser Irradiation
por: Qiao, Hongzhen, et al.
Publicado: (2018) -
Surface Quality and Material Removal Rate in Fabricating Microtexture on Tungsten Carbide via Femtosecond Laser
por: Li, Guangxian, et al.
Publicado: (2023)