Chemical behavior of aluminum and phosphorus during dissolution of glass fibers in physiological saline solutions.

The dissolution of textile glass fibers of four different compositions has been investigated at 37 degrees C. In these glasses, which are isolation type, the P2O5 contents scatter between 0 and 2 wt% and Al2O3 from 0.12 to 3.4 wt%. Both static (30-mg fibers; 250-ml solution) and dynamic (50-mg fiber...

Descripción completa

Detalles Bibliográficos
Autores principales: Baillif, P, Touray, J C
Formato: Texto
Lenguaje:English
Publicado: 1994
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC1567265/
https://www.ncbi.nlm.nih.gov/pubmed/7882961
_version_ 1782129791791529984
author Baillif, P
Touray, J C
author_facet Baillif, P
Touray, J C
author_sort Baillif, P
collection PubMed
description The dissolution of textile glass fibers of four different compositions has been investigated at 37 degrees C. In these glasses, which are isolation type, the P2O5 contents scatter between 0 and 2 wt% and Al2O3 from 0.12 to 3.4 wt%. Both static (30-mg fibers; 250-ml solution) and dynamic (50-mg fibers; 40 ml/day flow rate) conditions with or without bubbling of a gas mixture (95:5, N2-CO2) have been used. Two physiological solutions, one proposed by Kanapilly and the other by Scholtze, were used. After each run (1, 3, 7, 14, and sometimes 30, 62 days) the solutions were analyzed for B and Si by inductively coupled plasma (ICP), the weight losses were determined, and the residual solid were observed by scanning electron microscopy (SEM) and X-ray photoelectron spectroscopy (XPS). Static runs give a better agreement between measured and calculated weight losses from solution analyses than dynamic experiments. SEM examinations indicate diameter reduction and formation of a hydrated Si-rich layer. Sometimes hollow tubes, suggesting the detachment of these layers, are observed. XPS and energy dispersive X-ray (EDX) analysis indicate the formation of a veneer of calcium phosphate for the most rapidly dissolving glass. In other cases an Al increase is observed at the solid solution interface. Whatever experimental conditions are used, the relative dissolution rates of the four glasses are identical. The kinetics may be modeled with variable dissolution rates from initial high values to final low ones. The latter reflect the very low solubility of the residual product.
format Text
id pubmed-1567265
institution National Center for Biotechnology Information
language English
publishDate 1994
record_format MEDLINE/PubMed
spelling pubmed-15672652006-09-19 Chemical behavior of aluminum and phosphorus during dissolution of glass fibers in physiological saline solutions. Baillif, P Touray, J C Environ Health Perspect Research Article The dissolution of textile glass fibers of four different compositions has been investigated at 37 degrees C. In these glasses, which are isolation type, the P2O5 contents scatter between 0 and 2 wt% and Al2O3 from 0.12 to 3.4 wt%. Both static (30-mg fibers; 250-ml solution) and dynamic (50-mg fibers; 40 ml/day flow rate) conditions with or without bubbling of a gas mixture (95:5, N2-CO2) have been used. Two physiological solutions, one proposed by Kanapilly and the other by Scholtze, were used. After each run (1, 3, 7, 14, and sometimes 30, 62 days) the solutions were analyzed for B and Si by inductively coupled plasma (ICP), the weight losses were determined, and the residual solid were observed by scanning electron microscopy (SEM) and X-ray photoelectron spectroscopy (XPS). Static runs give a better agreement between measured and calculated weight losses from solution analyses than dynamic experiments. SEM examinations indicate diameter reduction and formation of a hydrated Si-rich layer. Sometimes hollow tubes, suggesting the detachment of these layers, are observed. XPS and energy dispersive X-ray (EDX) analysis indicate the formation of a veneer of calcium phosphate for the most rapidly dissolving glass. In other cases an Al increase is observed at the solid solution interface. Whatever experimental conditions are used, the relative dissolution rates of the four glasses are identical. The kinetics may be modeled with variable dissolution rates from initial high values to final low ones. The latter reflect the very low solubility of the residual product. 1994-10 /pmc/articles/PMC1567265/ /pubmed/7882961 Text en
spellingShingle Research Article
Baillif, P
Touray, J C
Chemical behavior of aluminum and phosphorus during dissolution of glass fibers in physiological saline solutions.
title Chemical behavior of aluminum and phosphorus during dissolution of glass fibers in physiological saline solutions.
title_full Chemical behavior of aluminum and phosphorus during dissolution of glass fibers in physiological saline solutions.
title_fullStr Chemical behavior of aluminum and phosphorus during dissolution of glass fibers in physiological saline solutions.
title_full_unstemmed Chemical behavior of aluminum and phosphorus during dissolution of glass fibers in physiological saline solutions.
title_short Chemical behavior of aluminum and phosphorus during dissolution of glass fibers in physiological saline solutions.
title_sort chemical behavior of aluminum and phosphorus during dissolution of glass fibers in physiological saline solutions.
topic Research Article
url https://www.ncbi.nlm.nih.gov/pmc/articles/PMC1567265/
https://www.ncbi.nlm.nih.gov/pubmed/7882961
work_keys_str_mv AT baillifp chemicalbehaviorofaluminumandphosphorusduringdissolutionofglassfibersinphysiologicalsalinesolutions
AT tourayjc chemicalbehaviorofaluminumandphosphorusduringdissolutionofglassfibersinphysiologicalsalinesolutions