Cargando…

Fluoride content and recharge ability of five glassionomer dental materials

BACKGROUND: The relationship between fluoride content and fluoride release for glass-ionomer cements is not well understood. The aim of this laboratory study was: to determine the fluoride concentrations at the surfaces of glass-ionomer materials with respect to different storage media and different...

Descripción completa

Detalles Bibliográficos
Autores principales: Markovic, Dejan Lj, Petrovic, Bojan B, Peric, Tamara O
Formato: Texto
Lenguaje:English
Publicado: BioMed Central 2008
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC2507707/
https://www.ncbi.nlm.nih.gov/pubmed/18655734
http://dx.doi.org/10.1186/1472-6831-8-21
_version_ 1782158389346828288
author Markovic, Dejan Lj
Petrovic, Bojan B
Peric, Tamara O
author_facet Markovic, Dejan Lj
Petrovic, Bojan B
Peric, Tamara O
author_sort Markovic, Dejan Lj
collection PubMed
description BACKGROUND: The relationship between fluoride content and fluoride release for glass-ionomer cements is not well understood. The aim of this laboratory study was: to determine the fluoride concentrations at the surfaces of glass-ionomer materials with respect to different storage media and different pH environments; to examine the recharge ability of the materials after NaF immersion; and to assess the morphological changes at the material surfaces using scanning electron microscope and energy dispersive spectroscopic techniques (SEM/EDS). METHODS: Five glass-ionomer materials, Fuji Triage (FT), Fuji II LC (FII), Fuji VIII (FVIII), Fuji IX GP (FIX), and Ketac N100 (KN), were analyzed in this study. Resin-based fluoride releasing material Helioseal F (HSF) was used as a comparison material. The sample consisted of 120 cured cement disks (n = 20 disks of each tested material, 10 × 1.5 mm). Five disks of each material were stored in 4 different storage media (I- saline, II- acidic solution ph = 2.5, III- acid solution ph = 5.5, IV- NaF solution (c = 500/106). After 7 days, two disks of each material were transferred from media I, II and III to the NaF solution for 3 min. EDS analysis was conducted in 3 randomly selected spots of each experimental disk. SEM was used to determine morphological characteristics of the material surface. Differences between the experimental groups have been analyzed using Student's t-test with the level of significance set at p < 0.001. RESULTS: FT showed the highest fluoride content at the surface of the material. The lowest amounts of fluoride ions were detected at the surfaces of the FT disks stored at low pH environments, and this difference was statistically significant (p < 0.001). Glass-ionomers showed significantly higher fluoride concentrations when compared to the HSF (p < 0.001). After immersion in the NaF solution, fluoride concentrations at the surfaces of the disks increased when compared with previous storage media (FT>FVIII>KN>FII>FIX). SEM analysis of the surface morphology revealed numerous voids, cracks and microporosities in all experimental groups, except for KN and HSF. More homogenous material structure with more discrete cracks was observed in samples stored at neutral pH environment, compared to disks stored in acidic solutions. CONCLUSION: The tested materials could be considered as promising dental materials with potential prophylactic characteristics due to their relatively high fluoride content, but also the ability to extensively reabsorb fluoride ions, especially in acidic environments.
format Text
id pubmed-2507707
institution National Center for Biotechnology Information
language English
publishDate 2008
publisher BioMed Central
record_format MEDLINE/PubMed
spelling pubmed-25077072008-08-12 Fluoride content and recharge ability of five glassionomer dental materials Markovic, Dejan Lj Petrovic, Bojan B Peric, Tamara O BMC Oral Health Research Article BACKGROUND: The relationship between fluoride content and fluoride release for glass-ionomer cements is not well understood. The aim of this laboratory study was: to determine the fluoride concentrations at the surfaces of glass-ionomer materials with respect to different storage media and different pH environments; to examine the recharge ability of the materials after NaF immersion; and to assess the morphological changes at the material surfaces using scanning electron microscope and energy dispersive spectroscopic techniques (SEM/EDS). METHODS: Five glass-ionomer materials, Fuji Triage (FT), Fuji II LC (FII), Fuji VIII (FVIII), Fuji IX GP (FIX), and Ketac N100 (KN), were analyzed in this study. Resin-based fluoride releasing material Helioseal F (HSF) was used as a comparison material. The sample consisted of 120 cured cement disks (n = 20 disks of each tested material, 10 × 1.5 mm). Five disks of each material were stored in 4 different storage media (I- saline, II- acidic solution ph = 2.5, III- acid solution ph = 5.5, IV- NaF solution (c = 500/106). After 7 days, two disks of each material were transferred from media I, II and III to the NaF solution for 3 min. EDS analysis was conducted in 3 randomly selected spots of each experimental disk. SEM was used to determine morphological characteristics of the material surface. Differences between the experimental groups have been analyzed using Student's t-test with the level of significance set at p < 0.001. RESULTS: FT showed the highest fluoride content at the surface of the material. The lowest amounts of fluoride ions were detected at the surfaces of the FT disks stored at low pH environments, and this difference was statistically significant (p < 0.001). Glass-ionomers showed significantly higher fluoride concentrations when compared to the HSF (p < 0.001). After immersion in the NaF solution, fluoride concentrations at the surfaces of the disks increased when compared with previous storage media (FT>FVIII>KN>FII>FIX). SEM analysis of the surface morphology revealed numerous voids, cracks and microporosities in all experimental groups, except for KN and HSF. More homogenous material structure with more discrete cracks was observed in samples stored at neutral pH environment, compared to disks stored in acidic solutions. CONCLUSION: The tested materials could be considered as promising dental materials with potential prophylactic characteristics due to their relatively high fluoride content, but also the ability to extensively reabsorb fluoride ions, especially in acidic environments. BioMed Central 2008-07-28 /pmc/articles/PMC2507707/ /pubmed/18655734 http://dx.doi.org/10.1186/1472-6831-8-21 Text en Copyright © 2008 Markovic et al; licensee BioMed Central Ltd. http://creativecommons.org/licenses/by/2.0 This is an Open Access article distributed under the terms of the Creative Commons Attribution License ( (http://creativecommons.org/licenses/by/2.0) ), which permits unrestricted use, distribution, and reproduction in any medium, provided the original work is properly cited.
spellingShingle Research Article
Markovic, Dejan Lj
Petrovic, Bojan B
Peric, Tamara O
Fluoride content and recharge ability of five glassionomer dental materials
title Fluoride content and recharge ability of five glassionomer dental materials
title_full Fluoride content and recharge ability of five glassionomer dental materials
title_fullStr Fluoride content and recharge ability of five glassionomer dental materials
title_full_unstemmed Fluoride content and recharge ability of five glassionomer dental materials
title_short Fluoride content and recharge ability of five glassionomer dental materials
title_sort fluoride content and recharge ability of five glassionomer dental materials
topic Research Article
url https://www.ncbi.nlm.nih.gov/pmc/articles/PMC2507707/
https://www.ncbi.nlm.nih.gov/pubmed/18655734
http://dx.doi.org/10.1186/1472-6831-8-21
work_keys_str_mv AT markovicdejanlj fluoridecontentandrechargeabilityoffiveglassionomerdentalmaterials
AT petrovicbojanb fluoridecontentandrechargeabilityoffiveglassionomerdentalmaterials
AT perictamarao fluoridecontentandrechargeabilityoffiveglassionomerdentalmaterials