AIM: The aim of this study was to test the hypothesis that bonding to caries-affected dentin would yield strengths that are lower than bond strengths achievable when bonded to normal dentin. Dentin-bonding systems used in this study were fourth and fifth generation as well as self-etching primers. M...

Descripción completa

Detalles Bibliográficos
Autores principales: Giriyappa, Ramesh H, Chandra, B Suresh
Formato: Texto
Lenguaje:English
Publicado: Medknow Publications 2008
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC2843536/
https://www.ncbi.nlm.nih.gov/pubmed/20351973
http://dx.doi.org/10.4103/0972-0707.48839
_version_ 1782179229825236992
author Giriyappa, Ramesh H
Chandra, B Suresh
author_facet Giriyappa, Ramesh H
Chandra, B Suresh
author_sort Giriyappa, Ramesh H
collection PubMed
description AIM: The aim of this study was to test the hypothesis that bonding to caries-affected dentin would yield strengths that are lower than bond strengths achievable when bonded to normal dentin. Dentin-bonding systems used in this study were fourth and fifth generation as well as self-etching primers. MATERIALS AND METHODS: Forty-eight freshly extracted mandibular and maxillary molars were selected of which 24 were caries-affected teeth and the remaining were noncarious teeth. Random sampling was done with eight teeth in each group based on the bonding system used. In caries-affected teeth, the soft, stainable, caries-infected dentin was excavated using a caries detector dye whereas the hard, caries-affected, nonstainable dentin was retained. All the teeth were subsequently mounted in a suitable acrylic mould. Prepared teeth were restored with a single composite resin, using three different dentin bonding systems. These prepared specimens were transferred to a Hounsfield tensometer to measure the shear bond strength. The results obtained were analyzed using Anova, Student's unpaired t-test, and Student Neuman Keulis test. RESULTS: The results showed that the self-etching primer required the highest mean shear load compared to the fifth and fourth generation dentin-bonding systems in both normal dentin and caries-affected dentin. CONCLUSION: Bond strength to dentin depends on whether the dentinal tubule is open or occluded. Within the limitations of this study, it was observed that bond strength to caries-affected dentin was low compared to normal dentin.
format Text
id pubmed-2843536
institution National Center for Biotechnology Information
language English
publishDate 2008
publisher Medknow Publications
record_format MEDLINE/PubMed
spelling pubmed-28435362010-03-26 Comparative evaluation of self-etching primers with fourth and fifth generation dentin-bonding systems on carious and normal dentin substrates: An in vitro shear bond strength analysis Giriyappa, Ramesh H Chandra, B Suresh J Conserv Dent Original Article AIM: The aim of this study was to test the hypothesis that bonding to caries-affected dentin would yield strengths that are lower than bond strengths achievable when bonded to normal dentin. Dentin-bonding systems used in this study were fourth and fifth generation as well as self-etching primers. MATERIALS AND METHODS: Forty-eight freshly extracted mandibular and maxillary molars were selected of which 24 were caries-affected teeth and the remaining were noncarious teeth. Random sampling was done with eight teeth in each group based on the bonding system used. In caries-affected teeth, the soft, stainable, caries-infected dentin was excavated using a caries detector dye whereas the hard, caries-affected, nonstainable dentin was retained. All the teeth were subsequently mounted in a suitable acrylic mould. Prepared teeth were restored with a single composite resin, using three different dentin bonding systems. These prepared specimens were transferred to a Hounsfield tensometer to measure the shear bond strength. The results obtained were analyzed using Anova, Student's unpaired t-test, and Student Neuman Keulis test. RESULTS: The results showed that the self-etching primer required the highest mean shear load compared to the fifth and fourth generation dentin-bonding systems in both normal dentin and caries-affected dentin. CONCLUSION: Bond strength to dentin depends on whether the dentinal tubule is open or occluded. Within the limitations of this study, it was observed that bond strength to caries-affected dentin was low compared to normal dentin. Medknow Publications 2008 /pmc/articles/PMC2843536/ /pubmed/20351973 http://dx.doi.org/10.4103/0972-0707.48839 Text en © Journal of Conservative Dentistry http://creativecommons.org/licenses/by/2.0/ This is an open-access article distributed under the terms of the Creative Commons Attribution License, which permits unrestricted use, distribution, and reproduction in any medium, provided the original work is properly cited.
spellingShingle Original Article
Giriyappa, Ramesh H
Chandra, B Suresh
Comparative evaluation of self-etching primers with fourth and fifth generation dentin-bonding systems on carious and normal dentin substrates: An in vitro shear bond strength analysis
title Comparative evaluation of self-etching primers with fourth and fifth generation dentin-bonding systems on carious and normal dentin substrates: An in vitro shear bond strength analysis
title_full Comparative evaluation of self-etching primers with fourth and fifth generation dentin-bonding systems on carious and normal dentin substrates: An in vitro shear bond strength analysis
title_fullStr Comparative evaluation of self-etching primers with fourth and fifth generation dentin-bonding systems on carious and normal dentin substrates: An in vitro shear bond strength analysis
title_full_unstemmed Comparative evaluation of self-etching primers with fourth and fifth generation dentin-bonding systems on carious and normal dentin substrates: An in vitro shear bond strength analysis
title_short Comparative evaluation of self-etching primers with fourth and fifth generation dentin-bonding systems on carious and normal dentin substrates: An in vitro shear bond strength analysis
title_sort comparative evaluation of self-etching primers with fourth and fifth generation dentin-bonding systems on carious and normal dentin substrates: an in vitro shear bond strength analysis
topic Original Article
url https://www.ncbi.nlm.nih.gov/pmc/articles/PMC2843536/
https://www.ncbi.nlm.nih.gov/pubmed/20351973
http://dx.doi.org/10.4103/0972-0707.48839
work_keys_str_mv AT giriyapparameshh comparativeevaluationofselfetchingprimerswithfourthandfifthgenerationdentinbondingsystemsoncariousandnormaldentinsubstratesaninvitroshearbondstrengthanalysis
AT chandrabsuresh comparativeevaluationofselfetchingprimerswithfourthandfifthgenerationdentinbondingsystemsoncariousandnormaldentinsubstratesaninvitroshearbondstrengthanalysis