Microscale wear behavior and crosslinking of PEG-like coatings for total hip replacements

The predominant cause of late-state failure of total hip replacements is wear-mediated osteolysis caused by wear particles that originate from the ultrahigh molecular weight polyethylene (UHMWPE) acetabular cup surface. One strategy for reducing wear particle formation from UHMWPE is to modify the s...

Descripción completa

Detalles Bibliográficos
Autores principales: Kane, Sheryl R., Ashby, Paul D., Pruitt, Lisa A.
Formato: Texto
Lenguaje:English
Publicado: Springer US 2009
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC2848970/
https://www.ncbi.nlm.nih.gov/pubmed/20091104
http://dx.doi.org/10.1007/s10856-009-3935-6
_version_ 1782179734357016576
author Kane, Sheryl R.
Ashby, Paul D.
Pruitt, Lisa A.
author_facet Kane, Sheryl R.
Ashby, Paul D.
Pruitt, Lisa A.
author_sort Kane, Sheryl R.
collection PubMed
description The predominant cause of late-state failure of total hip replacements is wear-mediated osteolysis caused by wear particles that originate from the ultrahigh molecular weight polyethylene (UHMWPE) acetabular cup surface. One strategy for reducing wear particle formation from UHMWPE is to modify the surface with a hydrophilic coating to increase lubrication from synovial fluid. This study focuses on the wear behavior of hydrophilic coatings similar to poly(ethylene glycol) (PEG). The coatings were produced by plasma-polymerizing tetraglyme on UHMWPE in a chamber heated to 40°C or 50°C. Both temperatures yielded coatings with PEG-like chemistry and increased hydrophilicity relative to uncoated UHMWPE; however, the 40°C coatings were significantly more resistant to damage induced by atomic force microscopy nanoscratching. The 40°C coatings exhibited only one damage mode (delamination) and often showed no signs of damage after repeated scratching. In contrast, the 50°C coatings exhibited three damage modes (roughening, thinning, and delamination), and always showed visible signs of damage after no more than two scratches. The greater wear resistance of the 40°C coatings could not be explained by coating chemistry or hydrophilicity, but it corresponded to an approximately 26–32% greater degree of crosslinking relative to the 50°C surfaces, suggesting that crosslinking should be a significant design consideration for hydrophilic coatings used for total hip replacements and other wear-dependent applications.
format Text
id pubmed-2848970
institution National Center for Biotechnology Information
language English
publishDate 2009
publisher Springer US
record_format MEDLINE/PubMed
spelling pubmed-28489702010-04-14 Microscale wear behavior and crosslinking of PEG-like coatings for total hip replacements Kane, Sheryl R. Ashby, Paul D. Pruitt, Lisa A. J Mater Sci Mater Med Article The predominant cause of late-state failure of total hip replacements is wear-mediated osteolysis caused by wear particles that originate from the ultrahigh molecular weight polyethylene (UHMWPE) acetabular cup surface. One strategy for reducing wear particle formation from UHMWPE is to modify the surface with a hydrophilic coating to increase lubrication from synovial fluid. This study focuses on the wear behavior of hydrophilic coatings similar to poly(ethylene glycol) (PEG). The coatings were produced by plasma-polymerizing tetraglyme on UHMWPE in a chamber heated to 40°C or 50°C. Both temperatures yielded coatings with PEG-like chemistry and increased hydrophilicity relative to uncoated UHMWPE; however, the 40°C coatings were significantly more resistant to damage induced by atomic force microscopy nanoscratching. The 40°C coatings exhibited only one damage mode (delamination) and often showed no signs of damage after repeated scratching. In contrast, the 50°C coatings exhibited three damage modes (roughening, thinning, and delamination), and always showed visible signs of damage after no more than two scratches. The greater wear resistance of the 40°C coatings could not be explained by coating chemistry or hydrophilicity, but it corresponded to an approximately 26–32% greater degree of crosslinking relative to the 50°C surfaces, suggesting that crosslinking should be a significant design consideration for hydrophilic coatings used for total hip replacements and other wear-dependent applications. Springer US 2009-12-20 2010 /pmc/articles/PMC2848970/ /pubmed/20091104 http://dx.doi.org/10.1007/s10856-009-3935-6 Text en © The Author(s) 2009 https://creativecommons.org/licenses/by-nc/4.0/ This article is distributed under the terms of the Creative Commons Attribution Noncommercial License which permits any noncommercial use, distribution, and reproduction in any medium, provided the original author(s) and source are credited.
spellingShingle Article
Kane, Sheryl R.
Ashby, Paul D.
Pruitt, Lisa A.
Microscale wear behavior and crosslinking of PEG-like coatings for total hip replacements
title Microscale wear behavior and crosslinking of PEG-like coatings for total hip replacements
title_full Microscale wear behavior and crosslinking of PEG-like coatings for total hip replacements
title_fullStr Microscale wear behavior and crosslinking of PEG-like coatings for total hip replacements
title_full_unstemmed Microscale wear behavior and crosslinking of PEG-like coatings for total hip replacements
title_short Microscale wear behavior and crosslinking of PEG-like coatings for total hip replacements
title_sort microscale wear behavior and crosslinking of peg-like coatings for total hip replacements
topic Article
url https://www.ncbi.nlm.nih.gov/pmc/articles/PMC2848970/
https://www.ncbi.nlm.nih.gov/pubmed/20091104
http://dx.doi.org/10.1007/s10856-009-3935-6
work_keys_str_mv AT kanesherylr microscalewearbehaviorandcrosslinkingofpeglikecoatingsfortotalhipreplacements
AT ashbypauld microscalewearbehaviorandcrosslinkingofpeglikecoatingsfortotalhipreplacements
AT pruittlisaa microscalewearbehaviorandcrosslinkingofpeglikecoatingsfortotalhipreplacements