Dielectric Relaxation of La-Doped Zirconia Caused by Annealing Ambient

La-doped zirconia films, deposited by ALD at 300°C, were found to be amorphous with dielectric constants (k-values) up to 19. A tetragonal or cubic phase was induced by post-deposition annealing (PDA) at 900°C in both nitrogen and air. Higher k-values (~32) were measured following PDA in air, but no...