Discovery of spontaneous deformation of Pd metal during hydrogen absorption/desorption cycles

A drastic deformation was observed in Pd metal of various shapes after hydrogen absorption and desorption cycles at 150 °C at a gas pressure of 1–5 MPa. All of the phenomena observed indicate that some strong internal force is induced spontaneously during hydrogen absorption/desorption cycles to pro...

Descripción completa

Detalles Bibliográficos
Autores principales: Yamazaki, Toshimitsu, Sato, Masaharu, Itoh, Satoshi
Formato: Online Artículo Texto
Lenguaje:English
Publicado: The Japan Academy 2009
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC3524300/
https://www.ncbi.nlm.nih.gov/pubmed/19444010
http://dx.doi.org/10.2183/pjab.85.183
Descripción
Sumario:A drastic deformation was observed in Pd metal of various shapes after hydrogen absorption and desorption cycles at 150 °C at a gas pressure of 1–5 MPa. All of the phenomena observed indicate that some strong internal force is induced spontaneously during hydrogen absorption/desorption cycles to produce a collective deformation so as to minimize the surface.