Cargando…
Discovery of spontaneous deformation of Pd metal during hydrogen absorption/desorption cycles
A drastic deformation was observed in Pd metal of various shapes after hydrogen absorption and desorption cycles at 150 °C at a gas pressure of 1–5 MPa. All of the phenomena observed indicate that some strong internal force is induced spontaneously during hydrogen absorption/desorption cycles to pro...
Autores principales: | Yamazaki, Toshimitsu, Sato, Masaharu, Itoh, Satoshi |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
The Japan Academy
2009
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC3524300/ https://www.ncbi.nlm.nih.gov/pubmed/19444010 http://dx.doi.org/10.2183/pjab.85.183 |
Ejemplares similares
-
The Structure Stability of Metal Diffusion Membrane-Filters in the Processes of Hydrogen Absorption/Desorption
por: Akimova, Olga V., et al.
Publicado: (2022) -
Preparation and Hydrogen Absorption/Desorption of Nanoporous Palladium Thin Films
por: Li, Wen-Chung, et al.
Publicado: (2009) -
Hydrogen absorption and desorption on Rh nanoparticles revealed by in situ dispersive X-ray absorption fine structure spectroscopy
por: Song, Chulho, et al.
Publicado: (2020) -
Catalytic Activities of Various Niobium Oxides for
Hydrogen Absorption/Desorption Reactions of Magnesium
por: Shinzato, Keita, et al.
Publicado: (2021) -
Graphene and Carbon Nanotubes Fibrous Composite Decorated with PdMg Alloy Nanoparticles with Enhanced Absorption–Desorption Kinetics for Hydrogen Storage Application
por: Arkook, Bassim, et al.
Publicado: (2021)