Cargando…

Phase Transformations of α-Alumina Made from Waste Aluminum via a Precipitation Technique

We report on a recycling project in which α-Al(2)O(3) was produced from aluminum cans because no such work has been reported in literature. Heated aluminum cans were mixed with 8.0 M of H(2)SO(4) solution to form an Al(2)(SO(4))(3) solution. The Al(2)(SO(4))(3) salt was contained in a white semi-liq...

Descripción completa

Detalles Bibliográficos
Autores principales: Matori, Khamirul Amin, Wah, Loy Chee, Hashim, Mansor, Ismail, Ismayadi, Zaid, Mohd Hafiz Mohd
Formato: Online Artículo Texto
Lenguaje:English
Publicado: Molecular Diversity Preservation International (MDPI) 2012
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC3546723/
https://www.ncbi.nlm.nih.gov/pubmed/23222685
http://dx.doi.org/10.3390/ijms131216812
Descripción
Sumario:We report on a recycling project in which α-Al(2)O(3) was produced from aluminum cans because no such work has been reported in literature. Heated aluminum cans were mixed with 8.0 M of H(2)SO(4) solution to form an Al(2)(SO(4))(3) solution. The Al(2)(SO(4))(3) salt was contained in a white semi-liquid solution with excess H(2)SO(4); some unreacted aluminum pieces were also present. The solution was filtered and mixed with ethanol in a ratio of 2:3, to form a white solid of Al(2)(SO(4))(3)·18H(2)O. The Al(2)(SO(4))(3)·18H(2)O was calcined in an electrical furnace for 3 h at temperatures of 400–1400 °C. The heating and cooling rates were 10 °C/min. XRD was used to investigate the phase changes at different temperatures and XRF was used to determine the elemental composition in the alumina produced. A series of different alumina compositions, made by repeated dehydration and desulfonation of the Al(2)(SO(4))(3)·18H(2)O, is reported. All transitional alumina phases produced at low temperatures were converted to α-Al(2)O(3) at high temperatures. The X-ray diffraction results indicated that the α-Al(2)O(3) phase was realized when the calcination temperature was at 1200 °C or higher.