Impact of oxalate desensitizer combined with ethylene-diamine tetra acetic acid-conditioning on dentin bond strength of one-bottle adhesives during dry bonding
BACKGROUND: Elimination of water entrapment in hybrid layer during bonding procedure would increase bonding durability. AIMS: This study evaluated the effect of oxalate desensitizer (OX) pretreatment on bond strength of three one-bottle adhesives to ethylene-diamine tetra acetic acid (EDTA)-conditio...
Autores principales: | , |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
Medknow Publications & Media Pvt Ltd
2013
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC3698591/ https://www.ncbi.nlm.nih.gov/pubmed/23833461 http://dx.doi.org/10.4103/0972-0707.111327 |
Sumario: | BACKGROUND: Elimination of water entrapment in hybrid layer during bonding procedure would increase bonding durability. AIMS: This study evaluated the effect of oxalate desensitizer (OX) pretreatment on bond strength of three one-bottle adhesives to ethylene-diamine tetra acetic acid (EDTA)-conditioned dentin under dry bonding. MATERIALS AND METHODS: Three adhesive systems, One-Step Plus (OS), Optibond Solo Plus (OP) and Adper Single Bond (SB) were bonded on dentin surfaces under four bonding conditions: (1) Wet-bonding on acid-etched dentin, (2) wet bonding on EDTA-conditioned dentin, (3) dry bonding on EDTA-conditioned dentin, (4) dry bonding associated with OX on the EDTA-conditioned dentin. After storage and thermo cycling, shear bond strength test was performed. Data were analyzed using two-way analysis of variance and Tukey tests. RESULTS: Wet bonding with EDTA or acid etching showed similar bond strength for test adhesives. Dry bonding with EDTA significantly decreased the bond strength of OS, but it had no effect on the bonding of OP and SB. OX application in the forth bonding condition, in comparison with the third condition, had a negative effect on the bond strength of OP, but not influence on OS and SB. CONCLUSIONS: The use of an OX on EDTA-conditioned dentin compromised the bonding efficacy of OS and OP under dry bonding but compatible for SB. |
---|