Cargando…
Adhesion of 10-MDP containing resin cements to dentin with and without the etch-and-rinse technique
PURPOSE: This study evaluated the adhesion of 10-MDP containing self-etch and self-adhesive resin cements to dentin with and without the use of etch-and-rinse technique. MATERIALS AND METHODS: Human third molars (N=180) were randomly divided into 6 groups (n=30 per group). Conventional (Panavia F2.0...
Autores principales: | , , , |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
The Korean Academy of Prosthodontics
2013
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC3774935/ https://www.ncbi.nlm.nih.gov/pubmed/24049562 http://dx.doi.org/10.4047/jap.2013.5.3.226 |
_version_ | 1782284543625003008 |
---|---|
author | Turp, Volkan Sen, Deniz Tuncelli, Betul Özcan, Mutlu |
author_facet | Turp, Volkan Sen, Deniz Tuncelli, Betul Özcan, Mutlu |
author_sort | Turp, Volkan |
collection | PubMed |
description | PURPOSE: This study evaluated the adhesion of 10-MDP containing self-etch and self-adhesive resin cements to dentin with and without the use of etch-and-rinse technique. MATERIALS AND METHODS: Human third molars (N=180) were randomly divided into 6 groups (n=30 per group). Conventional (Panavia F2.0, Kuraray-PAN) and self-adhesive resin cements (Clearfil SA, Kuraray-CSA) were bonded to dentin surfaces either after application of 3-step etch-and-rinse (35% H(3)PO(4) + ED Primer) or two-step self-etch adhesive resin (Clearfil SE Bond). Specimens were subjected to shear bond strength test using the universal testing machine (0.5 mm/min). The failure types were analyzed using a stereomicroscope and quality of hybrid layer was observed under a scanning electron microscope. The data (MPa) were analyzed using two-way ANOVA and Tukey's tests (α=.05). RESULTS: Overall, PAN adhesive cement showed significantly higher mean bond strength (12.5 ± 2.3 - 14.1 ± 2.4 MPa) than CSA cement (9.3 ± 1.4 - 13.9 ± 1.9 MPa) (P<.001). Adhesive failures were more frequent in CSA cement groups when used in conjunction with two-step self-adhesive (68%) or no adhesive at all (66%). Hybrid layer quality was inferior in CSA compared to PAN cement in all conditions. CONCLUSION: In clinical situations where bonding to dentin substrate is crucial, both conventional and self-adhesive resin cements based on 10-MDP can benefit from etch-and-rinse technique to achieve better quality of adhesion in the early clinical period. |
format | Online Article Text |
id | pubmed-3774935 |
institution | National Center for Biotechnology Information |
language | English |
publishDate | 2013 |
publisher | The Korean Academy of Prosthodontics |
record_format | MEDLINE/PubMed |
spelling | pubmed-37749352013-09-18 Adhesion of 10-MDP containing resin cements to dentin with and without the etch-and-rinse technique Turp, Volkan Sen, Deniz Tuncelli, Betul Özcan, Mutlu J Adv Prosthodont Original Article PURPOSE: This study evaluated the adhesion of 10-MDP containing self-etch and self-adhesive resin cements to dentin with and without the use of etch-and-rinse technique. MATERIALS AND METHODS: Human third molars (N=180) were randomly divided into 6 groups (n=30 per group). Conventional (Panavia F2.0, Kuraray-PAN) and self-adhesive resin cements (Clearfil SA, Kuraray-CSA) were bonded to dentin surfaces either after application of 3-step etch-and-rinse (35% H(3)PO(4) + ED Primer) or two-step self-etch adhesive resin (Clearfil SE Bond). Specimens were subjected to shear bond strength test using the universal testing machine (0.5 mm/min). The failure types were analyzed using a stereomicroscope and quality of hybrid layer was observed under a scanning electron microscope. The data (MPa) were analyzed using two-way ANOVA and Tukey's tests (α=.05). RESULTS: Overall, PAN adhesive cement showed significantly higher mean bond strength (12.5 ± 2.3 - 14.1 ± 2.4 MPa) than CSA cement (9.3 ± 1.4 - 13.9 ± 1.9 MPa) (P<.001). Adhesive failures were more frequent in CSA cement groups when used in conjunction with two-step self-adhesive (68%) or no adhesive at all (66%). Hybrid layer quality was inferior in CSA compared to PAN cement in all conditions. CONCLUSION: In clinical situations where bonding to dentin substrate is crucial, both conventional and self-adhesive resin cements based on 10-MDP can benefit from etch-and-rinse technique to achieve better quality of adhesion in the early clinical period. The Korean Academy of Prosthodontics 2013-08 2013-08-31 /pmc/articles/PMC3774935/ /pubmed/24049562 http://dx.doi.org/10.4047/jap.2013.5.3.226 Text en © 2013 The Korean Academy of Prosthodontics http://creativecommons.org/licenses/by-nc/3.0/ This is an Open Access article distributed under the terms of the Creative Commons Attribution Non-Commercial License (http://creativecommons.org/licenses/by-nc/3.0/) which permits unrestricted non-commercial use, distribution, and reproduction in any medium, provided the original work is properly cited. |
spellingShingle | Original Article Turp, Volkan Sen, Deniz Tuncelli, Betul Özcan, Mutlu Adhesion of 10-MDP containing resin cements to dentin with and without the etch-and-rinse technique |
title | Adhesion of 10-MDP containing resin cements to dentin with and without the etch-and-rinse technique |
title_full | Adhesion of 10-MDP containing resin cements to dentin with and without the etch-and-rinse technique |
title_fullStr | Adhesion of 10-MDP containing resin cements to dentin with and without the etch-and-rinse technique |
title_full_unstemmed | Adhesion of 10-MDP containing resin cements to dentin with and without the etch-and-rinse technique |
title_short | Adhesion of 10-MDP containing resin cements to dentin with and without the etch-and-rinse technique |
title_sort | adhesion of 10-mdp containing resin cements to dentin with and without the etch-and-rinse technique |
topic | Original Article |
url | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC3774935/ https://www.ncbi.nlm.nih.gov/pubmed/24049562 http://dx.doi.org/10.4047/jap.2013.5.3.226 |
work_keys_str_mv | AT turpvolkan adhesionof10mdpcontainingresincementstodentinwithandwithouttheetchandrinsetechnique AT sendeniz adhesionof10mdpcontainingresincementstodentinwithandwithouttheetchandrinsetechnique AT tuncellibetul adhesionof10mdpcontainingresincementstodentinwithandwithouttheetchandrinsetechnique AT ozcanmutlu adhesionof10mdpcontainingresincementstodentinwithandwithouttheetchandrinsetechnique |