Bond strength of veneer ceramic and zirconia cores with different surface modifications after microwave sintering

PURPOSE: To evaluate the effects of surface treatments on shear bond strength (SBS) between microwave and conventionally sintered zirconia core/veneers. MATERIALS AND METHODS: 96 disc shaped Noritake Alliance zirconia specimens were fabricated using YenaDent CAM unit and were divided in 2 groups wit...

Descripción completa

Detalles Bibliográficos
Autores principales: Saka, Muhammet, Yuzugullu, Bulem
Formato: Online Artículo Texto
Lenguaje:English
Publicado: The Korean Academy of Prosthodontics 2013
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC3865207/
https://www.ncbi.nlm.nih.gov/pubmed/24353890
http://dx.doi.org/10.4047/jap.2013.5.4.485
Descripción
Sumario:PURPOSE: To evaluate the effects of surface treatments on shear bond strength (SBS) between microwave and conventionally sintered zirconia core/veneers. MATERIALS AND METHODS: 96 disc shaped Noritake Alliance zirconia specimens were fabricated using YenaDent CAM unit and were divided in 2 groups with respect to microwave or conventional methods (n=48/group). Surface roughness (Ra) evaluation was made with a profilometer on randomly selected microwave (n=10) and conventionally sintered (n=10) cores. Specimens were then assessed into 4 subgroups according to surface treatments applied (n=12/group). Groups for microwave (M) and conventionally (C) sintered core specimens were as follows; M(C),C(C): untreated (control group), M(1),C(1):Al(2)O(3) sandblasting, M(2),C(2):liner, M(3),C(3):Al(2)O(3) sandblasting followed by liner. Veneer ceramic was fired on zirconia cores and specimens were thermocycled (6000 cycles between 5°-55℃). All specimens were subjected to SBS test using a universal testing machine at 0.5 mm/min, failure were evaluated under an optical microscope. Data were statistically analyzed using Shapiro Wilk, Levene, Post-hoc Tukey HSD and Student's t tests, Two-Way-Variance-Analysis and One-Way-Variance-Analysis (α=.05). RESULTS: Conventionally sintered specimens (1.06 ± 0.32 µm) showed rougher surfaces compared to microwave sintered ones (0.76 ± 0.32 µm)(P=.046), however, no correlation was found between SBS and surface roughness (r=-0.109, P=.658). The statistical comparison of the shear bond strengths of C(3) and C(1) group (P=.015); C(C) and M(C) group (P=.004) and C(3) and M(3) group presented statistically higher (P=.005) values. While adhesive failure was not seen in any of the groups, cohesive and combined patterns were seen in all groups. CONCLUSION: Based on the results of this in-vitro study, Al(2)O(3-) sandblasting followed by liner application on conventionally sintered zirconia cores may be preferred to enhance bond strength.