Six-month evaluation of a resin/dentin interface created by methacrylate and silorane-based materials

OBJECTIVES: This study aimed to compare the micro-tensile bond strength of methacrylate resin systems to a silorane-based restorative system on dentin after 24 hours and six months water storage. MATERIAL AND METHODS: The restorative systems Adper Single Bond 2/Filtek Z350 (ASB), Clearfil SE Bond/Z3...

Descripción completa

Detalles Bibliográficos
Autores principales: SAMPAIO, Renata Kirita Doi, WANG, Linda, de CARVALHO, Rodrigo Varella, GARCIA, Eugenio José, de ANDRADE, Andréa Mello, KLEIN-JÚNIOR, Celso Afonso, GRANDE, Rosa Helena Miranda, MOURA, Sandra Kiss
Formato: Online Artículo Texto
Lenguaje:English
Publicado: Faculdade de Odontologia de Bauru da Universidade de São Paulo 2013
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC3881815/
https://www.ncbi.nlm.nih.gov/pubmed/23559117
http://dx.doi.org/10.1590/1678-7757201302329
_version_ 1782298270402347008
author SAMPAIO, Renata Kirita Doi
WANG, Linda
de CARVALHO, Rodrigo Varella
GARCIA, Eugenio José
de ANDRADE, Andréa Mello
KLEIN-JÚNIOR, Celso Afonso
GRANDE, Rosa Helena Miranda
MOURA, Sandra Kiss
author_facet SAMPAIO, Renata Kirita Doi
WANG, Linda
de CARVALHO, Rodrigo Varella
GARCIA, Eugenio José
de ANDRADE, Andréa Mello
KLEIN-JÚNIOR, Celso Afonso
GRANDE, Rosa Helena Miranda
MOURA, Sandra Kiss
author_sort SAMPAIO, Renata Kirita Doi
collection PubMed
description OBJECTIVES: This study aimed to compare the micro-tensile bond strength of methacrylate resin systems to a silorane-based restorative system on dentin after 24 hours and six months water storage. MATERIAL AND METHODS: The restorative systems Adper Single Bond 2/Filtek Z350 (ASB), Clearfil SE Bond/Z350 (CF), Adper SE Plus/Z350 (ASEP) and P90 Adhesive System/Filtek P90 (P90) were applied on flat dentin surfaces of 20 third molars (n=5). The restored teeth were sectioned perpendicularly to the bonding interface to obtain sticks (0.8 mm(2)) to be tested after 24 hours (24 h) and 6 months (6 m) of water storage, in a universal testing machine at 0.5 mm/min. The data was analyzed via two-way Analysis of Variance/Bonferroni post hoc tests at 5% global significance. RESULTS: Overall outcomes did not indicate a statistical difference for the resin systems (p=0.26) nor time (p=0.62). No interaction between material x time was detected (p=0.28). Mean standard-deviation in MPa at 24 h and 6 m were: ASB 31.38 (4.53) and 30.06 (1.95), CF 34.26 (3.47) and 32.75 (4.18), ASEP 29.54 (4.14) and 33.47 (2.47), P90 30.27 (2.03) and 31.34 (2.19). CONCLUSIONS: The silorane-based system showed a similar performance to methacrylate-based materials on dentin. All systems were stable in terms of bond strength up to 6 month of water storage.
format Online
Article
Text
id pubmed-3881815
institution National Center for Biotechnology Information
language English
publishDate 2013
publisher Faculdade de Odontologia de Bauru da Universidade de São Paulo
record_format MEDLINE/PubMed
spelling pubmed-38818152014-01-08 Six-month evaluation of a resin/dentin interface created by methacrylate and silorane-based materials SAMPAIO, Renata Kirita Doi WANG, Linda de CARVALHO, Rodrigo Varella GARCIA, Eugenio José de ANDRADE, Andréa Mello KLEIN-JÚNIOR, Celso Afonso GRANDE, Rosa Helena Miranda MOURA, Sandra Kiss J Appl Oral Sci Original Articles OBJECTIVES: This study aimed to compare the micro-tensile bond strength of methacrylate resin systems to a silorane-based restorative system on dentin after 24 hours and six months water storage. MATERIAL AND METHODS: The restorative systems Adper Single Bond 2/Filtek Z350 (ASB), Clearfil SE Bond/Z350 (CF), Adper SE Plus/Z350 (ASEP) and P90 Adhesive System/Filtek P90 (P90) were applied on flat dentin surfaces of 20 third molars (n=5). The restored teeth were sectioned perpendicularly to the bonding interface to obtain sticks (0.8 mm(2)) to be tested after 24 hours (24 h) and 6 months (6 m) of water storage, in a universal testing machine at 0.5 mm/min. The data was analyzed via two-way Analysis of Variance/Bonferroni post hoc tests at 5% global significance. RESULTS: Overall outcomes did not indicate a statistical difference for the resin systems (p=0.26) nor time (p=0.62). No interaction between material x time was detected (p=0.28). Mean standard-deviation in MPa at 24 h and 6 m were: ASB 31.38 (4.53) and 30.06 (1.95), CF 34.26 (3.47) and 32.75 (4.18), ASEP 29.54 (4.14) and 33.47 (2.47), P90 30.27 (2.03) and 31.34 (2.19). CONCLUSIONS: The silorane-based system showed a similar performance to methacrylate-based materials on dentin. All systems were stable in terms of bond strength up to 6 month of water storage. Faculdade de Odontologia de Bauru da Universidade de São Paulo 2013 /pmc/articles/PMC3881815/ /pubmed/23559117 http://dx.doi.org/10.1590/1678-7757201302329 Text en http://creativecommons.org/licenses/by-nc/3.0/ This is an Open Access article distributed under the terms of the Creative Commons Attribution Non-Commercial License which permits unrestricted non-commercial use, distribution, and reproduction in any medium, provided the original work is properly cited.
spellingShingle Original Articles
SAMPAIO, Renata Kirita Doi
WANG, Linda
de CARVALHO, Rodrigo Varella
GARCIA, Eugenio José
de ANDRADE, Andréa Mello
KLEIN-JÚNIOR, Celso Afonso
GRANDE, Rosa Helena Miranda
MOURA, Sandra Kiss
Six-month evaluation of a resin/dentin interface created by methacrylate and silorane-based materials
title Six-month evaluation of a resin/dentin interface created by methacrylate and silorane-based materials
title_full Six-month evaluation of a resin/dentin interface created by methacrylate and silorane-based materials
title_fullStr Six-month evaluation of a resin/dentin interface created by methacrylate and silorane-based materials
title_full_unstemmed Six-month evaluation of a resin/dentin interface created by methacrylate and silorane-based materials
title_short Six-month evaluation of a resin/dentin interface created by methacrylate and silorane-based materials
title_sort six-month evaluation of a resin/dentin interface created by methacrylate and silorane-based materials
topic Original Articles
url https://www.ncbi.nlm.nih.gov/pmc/articles/PMC3881815/
https://www.ncbi.nlm.nih.gov/pubmed/23559117
http://dx.doi.org/10.1590/1678-7757201302329
work_keys_str_mv AT sampaiorenatakiritadoi sixmonthevaluationofaresindentininterfacecreatedbymethacrylateandsiloranebasedmaterials
AT wanglinda sixmonthevaluationofaresindentininterfacecreatedbymethacrylateandsiloranebasedmaterials
AT decarvalhorodrigovarella sixmonthevaluationofaresindentininterfacecreatedbymethacrylateandsiloranebasedmaterials
AT garciaeugeniojose sixmonthevaluationofaresindentininterfacecreatedbymethacrylateandsiloranebasedmaterials
AT deandradeandreamello sixmonthevaluationofaresindentininterfacecreatedbymethacrylateandsiloranebasedmaterials
AT kleinjuniorcelsoafonso sixmonthevaluationofaresindentininterfacecreatedbymethacrylateandsiloranebasedmaterials
AT granderosahelenamiranda sixmonthevaluationofaresindentininterfacecreatedbymethacrylateandsiloranebasedmaterials
AT mourasandrakiss sixmonthevaluationofaresindentininterfacecreatedbymethacrylateandsiloranebasedmaterials