Negative Effect of Rapidly Resorbing Properties of Bioactive Glass-Ceramics as Bone Graft Substitute in a Rabbit Lumbar Fusion Model

BACKGROUND: Bioactive glass-ceramics have the ability to directly bind to bones and have been widely used as bone graft substitutes due to their high osteoconductivity and biocompatibility. CaO-SiO(2)-P(2)O(5)-B(2)O(3) glass-ceramics are known to have good osteoconductivity and are used as bone graf...

Descripción completa

Detalles Bibliográficos
Autores principales: Lee, Jae Hyup, Ryu, Hyun-Seung, Seo, Jun-Hyuk, Lee, Do-Yoon, Chang, Bong-Soon, Lee, Choon-Ki
Formato: Online Artículo Texto
Lenguaje:English
Publicado: The Korean Orthopaedic Association 2014
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC3942607/
https://www.ncbi.nlm.nih.gov/pubmed/24605194
http://dx.doi.org/10.4055/cios.2014.6.1.87
Descripción
Sumario:BACKGROUND: Bioactive glass-ceramics have the ability to directly bind to bones and have been widely used as bone graft substitutes due to their high osteoconductivity and biocompatibility. CaO-SiO(2)-P(2)O(5)-B(2)O(3) glass-ceramics are known to have good osteoconductivity and are used as bone graft extenders. METHODS: This study aimed to evaluate the effects of the resorbing properties of glass-ceramics in bone fusion after producing and analyzing three types of CaO-SiO(2)-P(2)O(5)-B(2)O(3) glass-ceramics with high osteoconductivity that had enhanced resorption by having an increased B(2)O(3) content. The three types of CaO-SiO(2)-P(2)O(5)-B(2)O(3) glass-ceramics with B(2)O(3) contents of 8.0, 9.0, and 9.5 weight % were designated and grouped as P20B80, P10B90, and P5B95, respectively. Glass-ceramic types were tested for fusion rates and bone formation by employing the lumbar 5-6 intertransverse process fusion model in 51 New Zealand male rabbits. Bioactivity was assessed by soaking in simulated body fluid (SBF). RESULTS: In vitro study results showed sufficient hydroxycarbonate apatite layer formation occurred for P20B80 in1 day, for P10B90 in 3 days, and for P5B95 in 5 days after soaking in SBF. For the rabbit lumbar spine posterolateral fusion model, the autograft group recorded a 100% fusion rate with levels significantly higher than those of P20B80 (29.4%), P10B90 (0%), and P5B95 (14.3%), with high resorbing properties. Resorbing property differences among the three glass-ceramic groups were not significant. Histological results showed new bone formation confirming osteoconductivity in all three types of glass-ceramics. Radiomorphometric results also confirmed the resorbing properties of the three glass-ceramic types. CONCLUSIONS: The high resorbing properties and osteoconductivity of porous glass-ceramics can be advantageous as no glass-ceramics remain in the body. However, their relatively fast rate of resorption in the body negatively affects their role as an osteoconductive scaffold as glass-ceramics are resorbed before bony fusion.