The Effect of Prophylactic Polishing Pastes on Surface Roughness of Indirect Restorative Materials

The purpose of this study was to evaluate the influence of prophylactic polishing pastes (PPP; Detartrine (DT), Topex (TP)) on surface roughness (R (a)) of indirect composites (IRC; Tescera (TES), Gradia (GRD), and Estenia C&B (EST)), a glass ceramic (Empress 2 layering (E2)), and a leucite rein...

Descripción completa

Detalles Bibliográficos
Autores principales: Can Say, Esra, Yurdagüven, Haktan, Malkondu, Özlem, Ünlü, Nimet, Soyman, Mübin, Kazazoğlu, Ender
Formato: Online Artículo Texto
Lenguaje:English
Publicado: Hindawi Publishing Corporation 2014
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC3960528/
https://www.ncbi.nlm.nih.gov/pubmed/24729757
http://dx.doi.org/10.1155/2014/962764
Descripción
Sumario:The purpose of this study was to evaluate the influence of prophylactic polishing pastes (PPP; Detartrine (DT), Topex (TP)) on surface roughness (R (a)) of indirect composites (IRC; Tescera (TES), Gradia (GRD), and Estenia C&B (EST)), a glass ceramic (Empress 2 layering (E2)), and a leucite reinforced glass ceramic (Empress Esthetic (EE)) with two different (glazed (G); polished (P)) surface preparations. A total of 90 IRC and 120 ceramic discs, 8 mm in diameter and 2 mm thick, were prepared. E2 and EE specimens were randomly divided into two groups (n = 30). One group was glazed (GE2; GEE), while the other group was polished (PE2; PEE) the same as the IRCs. The specimens in each group were subsequently divided into three subgroups: control (C), DT, and TP. R (a) (μm) was evaluated with a profilometer. Data were analyzed by Kruskal Wallis, followed by the Dunn's multiple comparison tests (P < 0.05). DT and TP resulted in significant surface roughening for TES, GRD, and EST, while no significant differences were detected between DT and TP (P > 0.05). PE2 and PEE were not affected by DT or TP (P > 0.05), while GE2 and GEE exhibited significant roughening after TP (P < 0.05). Surface roughness of IRCs and glazed ceramics can be affected by PPP applications.