Cargando…

Size-Dependent MRI Relaxivity and Dual Imaging with Eu(0.2)Gd(0.8)PO(4)·H(2)O Nanoparticles

[Image: see text] Three different sizes of Eu(0.2)Gd(0.8)PO(4)·H(2)O nanoparticles have been prepared to investigate the particle size influence on water proton relaxivity. Longitudinal relaxivity (r(1)) values increase for smaller particles, reaching as high as r(1) = 6.13 mM(–1) s(–1) for a sample...

Descripción completa

Detalles Bibliográficos
Autores principales: Li, Yichen, Chen, Tao, Tan, Weihong, Talham, Daniel R.
Formato: Online Artículo Texto
Lenguaje:English
Publicado: American Chemical Society 2014
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC4039354/
https://www.ncbi.nlm.nih.gov/pubmed/24825171
http://dx.doi.org/10.1021/la500602x