Reliable coupling of orthodontic elements to mini-implants: An in-vitro study

OBJECTIVES: To investigate the reliability of mechanical and adhesive methods of fixing rectangular wires in the cross-slot of a mini-implant. MATERIALS AND METHODS: A twin-hooked wire element was placed and fixed in the slot of a mini-implant via a NiTi spring under tension, or by means of an adhes...

Descripción completa

Detalles Bibliográficos
Autores principales: Ludwig, Björn, Zipprich, Holger, Gebel, Britta, Piller, Ben, Antoszewska, Joanna
Formato: Online Artículo Texto
Lenguaje:English
Publicado: Medknow Publications & Media Pvt Ltd 2012
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC4072352/
https://www.ncbi.nlm.nih.gov/pubmed/24987620
http://dx.doi.org/10.4103/2278-0203.94774
Descripción
Sumario:OBJECTIVES: To investigate the reliability of mechanical and adhesive methods of fixing rectangular wires in the cross-slot of a mini-implant. MATERIALS AND METHODS: A twin-hooked wire element was placed and fixed in the slot of a mini-implant via a NiTi spring under tension, or by means of an adhesive. For the purpose of mechanical anchorage, the wire was crimped with a special crimping tool to increase its thickness and prevent it from slipping through the slot. Before applying the adhesive, there were four possible methods of preparation: Untreated Wire (Adh. 1); ROCATEC-Pre (Adh. 2); ROCATEC-PRE + Espe Sil (Adh. 3); ROCATEC-PRE + ROCATEC-PLUS + Espe Sil (Adh. 4). The mechanical fixing and two adhesive fixings were aged by means of temperature change (500 cycles). A Zwick universal testing machine was used to measure the maximum strength of the coupling. RESULTS: In all tests, the untreated wire + adhesive withstood the lowest maximum load (Ø 3 N and 10.8 N respectively) and failed the aging test after a maximum of eight cycles. The wires in test group Adh. 4 withstood the highest maximum load (Ø 43.3 N; 41.5 N; 45.9 N after aging) in all tests. The average load withstood by the crimped ligature was 38.7 N. CONCLUSION: The adhesive method of fixation performs best when the rectangular wire is sand blasted and silanized before application. The mechanical coupling using the crimped ligature is reliable.