The assessment of surface roughness and microleakage of eroded tooth-colored dental restorative materials
OBJECTIVES: To investigate the effect of acidic solution on surface roughness and microleakage of tooth-colored restorative materials. MATERIALS AND METHODS: A 160 box-shaped cavities were prepared on the buccal surfaces of 160 human molars, and assigned to four groups: Group A restored with Ketac™...
Autores principales: | , , , |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
Medknow Publications & Media Pvt Ltd
2014
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC4252925/ https://www.ncbi.nlm.nih.gov/pubmed/25506139 http://dx.doi.org/10.4103/0972-0707.144585 |
_version_ | 1782347201219919872 |
---|---|
author | Hussein, Thulfiqar Ali Bakar, Wan Zaripah Wan Ghani, Zuryati Ab Mohamad, Dasmawati |
author_facet | Hussein, Thulfiqar Ali Bakar, Wan Zaripah Wan Ghani, Zuryati Ab Mohamad, Dasmawati |
author_sort | Hussein, Thulfiqar Ali |
collection | PubMed |
description | OBJECTIVES: To investigate the effect of acidic solution on surface roughness and microleakage of tooth-colored restorative materials. MATERIALS AND METHODS: A 160 box-shaped cavities were prepared on the buccal surfaces of 160 human molars, and assigned to four groups: Group A restored with Ketac™ Molar Easymix, Group B with Fuji II™ LC, Group C with Ketac™ N100, and Group D with Filtek™ Z250, and subdivided into study and control groups (n = 20). Study groups were immersed in lemon juice (pH = 2.79) for 24 h, whilst controlgroups in deionized distilled water. All samples were immersed in 2% methylene blue dye, sectioned into two equal halves for surface roughness, and microleakage tests. Data were analyzed using Mann–Whitney and Kruskal–Wallis tests at P < 0.05. RESULTS: There was a significant difference in surface roughness of Ketac™ Molar, Fuji II™ LC, and Ketac™ N100. No significant difference was found in microleakage of Ketac™ Molar and Fuji II™ LC; however, there were significant differences in the gingival margin of Ketac™ N100, and the occlusal margin of Filtek™ Z250. CONCLUSIONS: All glass ionomer cements were eroded after exposure to the acidic drink. Filtek™ Z250 and Ketac™ Molar Easymix showed more microleakage. All materials showed more microleakage at the gingival margins. |
format | Online Article Text |
id | pubmed-4252925 |
institution | National Center for Biotechnology Information |
language | English |
publishDate | 2014 |
publisher | Medknow Publications & Media Pvt Ltd |
record_format | MEDLINE/PubMed |
spelling | pubmed-42529252014-12-12 The assessment of surface roughness and microleakage of eroded tooth-colored dental restorative materials Hussein, Thulfiqar Ali Bakar, Wan Zaripah Wan Ghani, Zuryati Ab Mohamad, Dasmawati J Conserv Dent Original Article OBJECTIVES: To investigate the effect of acidic solution on surface roughness and microleakage of tooth-colored restorative materials. MATERIALS AND METHODS: A 160 box-shaped cavities were prepared on the buccal surfaces of 160 human molars, and assigned to four groups: Group A restored with Ketac™ Molar Easymix, Group B with Fuji II™ LC, Group C with Ketac™ N100, and Group D with Filtek™ Z250, and subdivided into study and control groups (n = 20). Study groups were immersed in lemon juice (pH = 2.79) for 24 h, whilst controlgroups in deionized distilled water. All samples were immersed in 2% methylene blue dye, sectioned into two equal halves for surface roughness, and microleakage tests. Data were analyzed using Mann–Whitney and Kruskal–Wallis tests at P < 0.05. RESULTS: There was a significant difference in surface roughness of Ketac™ Molar, Fuji II™ LC, and Ketac™ N100. No significant difference was found in microleakage of Ketac™ Molar and Fuji II™ LC; however, there were significant differences in the gingival margin of Ketac™ N100, and the occlusal margin of Filtek™ Z250. CONCLUSIONS: All glass ionomer cements were eroded after exposure to the acidic drink. Filtek™ Z250 and Ketac™ Molar Easymix showed more microleakage. All materials showed more microleakage at the gingival margins. Medknow Publications & Media Pvt Ltd 2014 /pmc/articles/PMC4252925/ /pubmed/25506139 http://dx.doi.org/10.4103/0972-0707.144585 Text en Copyright: © Journal of Conservative Dentistry http://creativecommons.org/licenses/by-nc-sa/3.0 This is an open-access article distributed under the terms of the Creative Commons Attribution-Noncommercial-Share Alike 3.0 Unported, which permits unrestricted use, distribution, and reproduction in any medium, provided the original work is properly cited. |
spellingShingle | Original Article Hussein, Thulfiqar Ali Bakar, Wan Zaripah Wan Ghani, Zuryati Ab Mohamad, Dasmawati The assessment of surface roughness and microleakage of eroded tooth-colored dental restorative materials |
title | The assessment of surface roughness and microleakage of eroded tooth-colored dental restorative materials |
title_full | The assessment of surface roughness and microleakage of eroded tooth-colored dental restorative materials |
title_fullStr | The assessment of surface roughness and microleakage of eroded tooth-colored dental restorative materials |
title_full_unstemmed | The assessment of surface roughness and microleakage of eroded tooth-colored dental restorative materials |
title_short | The assessment of surface roughness and microleakage of eroded tooth-colored dental restorative materials |
title_sort | assessment of surface roughness and microleakage of eroded tooth-colored dental restorative materials |
topic | Original Article |
url | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC4252925/ https://www.ncbi.nlm.nih.gov/pubmed/25506139 http://dx.doi.org/10.4103/0972-0707.144585 |
work_keys_str_mv | AT husseinthulfiqarali theassessmentofsurfaceroughnessandmicroleakageoferodedtoothcoloreddentalrestorativematerials AT bakarwanzaripahwan theassessmentofsurfaceroughnessandmicroleakageoferodedtoothcoloreddentalrestorativematerials AT ghanizuryatiab theassessmentofsurfaceroughnessandmicroleakageoferodedtoothcoloreddentalrestorativematerials AT mohamaddasmawati theassessmentofsurfaceroughnessandmicroleakageoferodedtoothcoloreddentalrestorativematerials AT husseinthulfiqarali assessmentofsurfaceroughnessandmicroleakageoferodedtoothcoloreddentalrestorativematerials AT bakarwanzaripahwan assessmentofsurfaceroughnessandmicroleakageoferodedtoothcoloreddentalrestorativematerials AT ghanizuryatiab assessmentofsurfaceroughnessandmicroleakageoferodedtoothcoloreddentalrestorativematerials AT mohamaddasmawati assessmentofsurfaceroughnessandmicroleakageoferodedtoothcoloreddentalrestorativematerials |