Sessile dislocations by reactions in NiAl severely deformed at room temperature
B2 ordered NiAl is known for its poor room temperature (RT) ductility; failure occurs in a brittle like manner even in ductile single crystals deforming by single slip. In the present study NiAl was severely deformed at RT using the method of high pressure torsion (HPT) enabling the hitherto impossi...
Autores principales: | Geist, D., Gammer, C., Rentenberger, C., Karnthaler, H.P. |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
Elsevier
2015
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC4308006/ https://www.ncbi.nlm.nih.gov/pubmed/25663749 http://dx.doi.org/10.1016/j.jallcom.2014.09.226 |
Ejemplares similares
-
Structural modifications during heating of bulk nanocrystalline FeAl produced by high-pressure torsion
por: Mangler, C., et al.
Publicado: (2010) -
Shift of Creep Mechanism in Nanocrystalline NiAl Alloy
por: Sun, Zhihui, et al.
Publicado: (2019) -
Influence of the Ag concentration on the medium-range order in a CuZrAlAg bulk metallic glass
por: Gammer, C., et al.
Publicado: (2017) -
Synthesis of NiAl Intermetallic Compound under Shock-Wave Extrusion
por: Malakhov, Andrey, et al.
Publicado: (2022) -
Expanded graphite/NiAl layered double hydroxide nanowires for ultra-sensitive, ultra-low detection limits and selective NO(x) gas detection at room temperature
por: Zhang, Xueying, et al.
Publicado: (2019)