Comparison of growth texture in round Bi2212 and flat Bi2223 wires and its relation to high critical current density development
Why Bi(2)Sr(2)CaCu(2)O(x) (Bi2212) allows high critical current density J(c) in round wires rather than only in the anisotropic tape form demanded by all other high temperature superconductors is important for future magnet applications. Here we compare the local texture of state-of-the-art Bi2212 a...
Autores principales: | Kametani, F., Jiang, J., Matras, M., Abraimov, D., Hellstrom, E. E., Larbalestier, D. C. |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
Nature Publishing Group
2015
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC4322349/ https://www.ncbi.nlm.nih.gov/pubmed/25666114 http://dx.doi.org/10.1038/srep08285 |
Ejemplares similares
-
Correlation of critical current density to quasi-biaxial texture and grain boundary cleanliness in fully dense Bi-2212 wires
por: Oloye, T A, et al.
Publicado: (2021) -
Reduction of Gas Bubbles and Improved Critical Current Density in Bi-2212 Round Wire by Swaging
por: Jiang, J, et al.
Publicado: (2013) -
Bubble Formation within Filaments of Melt-Processed Bi2212 wires and its strongly negative effect on the Critical Current Density
por: Kametani, F, et al.
Publicado: (2011) -
Strain induced irreversible critical current degradation in highly dense Bi-2212 round wire
por: Bjoerstad, R, et al.
Publicado: (2015) -
Influence of the oxygen partial pressure on the phase evolution during Bi-2212 wire melt processing
por: Scheuerlein, C., et al.