Large increase in fracture resistance of stishovite with crack extension less than one micrometer
The development of strong, tough, and damage-tolerant ceramics requires nano/microstructure design to utilize toughening mechanisms operating at different length scales. The toughening mechanisms so far known are effective in micro-scale, then, they require the crack extension of more than a few mic...
Autores principales: | Yoshida, Kimiko, Wakai, Fumihiro, Nishiyama, Norimasa, Sekine, Risako, Shinoda, Yutaka, Akatsu, Takashi, Nagoshi, Takashi, Sone, Masato |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
Nature Publishing Group
2015
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC4458880/ https://www.ncbi.nlm.nih.gov/pubmed/26051871 http://dx.doi.org/10.1038/srep10993 |
Ejemplares similares
-
Picosecond amorphization of SiO(2) stishovite under tension
por: Misawa, Masaaki, et al.
Publicado: (2017) -
Fracture-induced amorphization of polycrystalline SiO(2) stishovite: a potential platform for toughening in ceramics
por: Nishiyama, Norimasa, et al.
Publicado: (2014) -
Effect of the Elastic Deformation of a Point-Sharp Indenter on Nanoindentation Behavior
por: Akatsu, Takashi, et al.
Publicado: (2017) -
Effect of Equibiaxial Pre-Stress on Mechanical Properties Evaluated Using Depth-Sensing Indentation with a Point-Sharp Indenter
por: Akatsu, Takashi, et al.
Publicado: (2023) -
Muonium in Stishovite: Implications for the Possible Existence of Neutral Atomic Hydrogen in the Earth's Deep Mantle
por: Funamori, Nobumasa, et al.
Publicado: (2015)