Enhanced Photoelectrochemical Activity of ZnO-Coated TiO(2) Nanotubes and Its Dependence on ZnO Coating Thickness
One-dimensional heterogeneous nanostructures in the form of ZnO-coated TiO(2) nanotubes (ZnO/TiO(2) NTs) were fabricated by atomic layer deposition of an ultrathin ZnO coating on electrochemical anodization-formed TiO(2) nanotubes (NTs) with the thickness of ZnO coating being precisely controlled at...
Autores principales: | , , , , , , , |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
Springer US
2016
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC4766178/ https://www.ncbi.nlm.nih.gov/pubmed/26911568 http://dx.doi.org/10.1186/s11671-016-1309-9 |
Sumario: | One-dimensional heterogeneous nanostructures in the form of ZnO-coated TiO(2) nanotubes (ZnO/TiO(2) NTs) were fabricated by atomic layer deposition of an ultrathin ZnO coating on electrochemical anodization-formed TiO(2) nanotubes (NTs) with the thickness of ZnO coating being precisely controlled at atomic scale, and the photoelectrochemical activity of the fabricated ZnO/TiO(2) NTs and the influence of ZnO coating and its thickness were studied. The structures of TiO(2) NTs and ZnO coatings were characterized by X-ray diffraction, Raman backscattering spectroscopy, and transmission electron microscopy. The photoelectrochemical activity was studied through the measurements of electrochemical impendence, flat-band potential, and transient photocurrent density. The TiO(2) NTs exhibit anatase structure, and the ZnO coatings are structured with hexagonal wurtzite. The photoelectrochemical activity of the ZnO/TiO(2) NTs is strongly dependent on the thickness of ZnO coating. ZnO/TiO(2) NTs with a thinner rather than a thicker ZnO coating exhibit better photoelectrochemical activity with reduced charge transfer resistance, increased negative flat-band potentials, and enhanced photocurrent densities. Under visible illumination, an increase of about 60 % in the photoelectrochemical activity is obtained for ZnO/TiO(2) NTs with an about 2-nm-thick ZnO coating. |
---|