Cargando…
Oxidation Resistance of Materials Based on Ti(3)AlC(2) Nanolaminate at 600 °C in Air
The oxidation behavior of Ti(3)AlC(2)-based materials had been investigated at 600 °C in static air for 1000 h. It was shown that the intense increase of weight gain per unit surface area for sintered material with porosity of 22 % attributed to oxidation of the outer surface of the specimen and sur...
Autores principales: | Ivasyshyn, Andrij, Ostash, Orest, Prikhna, Tatiana, Podhurska, Viktoriya, Basyuk, Tatiana |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
Springer US
2016
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC4978654/ https://www.ncbi.nlm.nih.gov/pubmed/27506531 http://dx.doi.org/10.1186/s11671-016-1571-x |
Ejemplares similares
-
Preconditioning of the YSZ-NiO Fuel Cell Anode in Hydrogenous Atmospheres Containing Water Vapor
por: Vasyliv, Bogdan, et al.
Publicado: (2017) -
Influence of Treatment Temperature on Microstructure and Properties of YSZ–NiO Anode Materials
por: Podhurska, Viktoriya, et al.
Publicado: (2016) -
Effects of Al substitution by Si in Ti(3)AlC(2) nanolaminate
por: Hadi, M. A., et al.
Publicado: (2021) -
On the stochastic phase stability of Ti(2)AlC-Cr(2)AlC
por: Duong, Thien C., et al.
Publicado: (2017) -
Transparent and flexible capacitors based on nanolaminate Al(2)O(3)/TiO(2)/Al(2)O(3)
por: Zhang, Guozhen, et al.
Publicado: (2015)