Texture design for microwave dielectric (Ca(0.7)Nd(0.3))(0.87)TiO(3) ceramics through reactive-templated grain growth
Plate-like Ca(3)Ti(2)O(7) (CT) and Nd(2)Ti(2)O(7) (NT) particles were synthesized in molten salts and used as reactive templates for the preparation of highly textured (Ca(0.7)Nd(0.3))(0.87)TiO(3) bulk ceramics (CNT) with preferred pseudocubic 〈100〉 and 〈110〉 orientations, respectively. During flux...
Autores principales: | Tani, Toshihiko, Takeuchi, Tsuguto |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
Taylor & Francis
2015
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC5099846/ https://www.ncbi.nlm.nih.gov/pubmed/27877809 http://dx.doi.org/10.1088/1468-6996/16/3/035008 |
Ejemplares similares
-
Thickness-dependent electrocaloric effect in mixed-phase Pb(0.87)Ba(0.1) La(0.02)(Zr(0.6)Sn(0.33)Ti(0.07))O(3) thin films
por: Correia, T. M., et al.
Publicado: (2016) -
Influence of Grain Size on Dielectric Behavior in Lead-Free 0.5 Ba(Zr(0.2)Ti(0.8))O(3)–0.5 (Ba(0.7)Ca(0.3))TiO(3) Ceramics
por: Ene, Vladimir Lucian, et al.
Publicado: (2023) -
Manipulating magnetoelectric properties by interfacial coupling in La(0.3)Sr(0.7)MnO(3)/Ba(0.7)Sr(0.3)TiO(3) superlattices
por: Guo, Haizhong, et al.
Publicado: (2017) -
Magnetocapacitance in La(0.7)Sr(0.3)MnO(3)/Pb(Zr(0.2)Ti(0.8))O(3)/La(0.7)Sr(0.3)MnO(3) multiferroic heterostructures
por: Hrib, Luminita M., et al.
Publicado: (2017) -
Temperature-Driven Transformation of the Crystal and Magnetic Structures of BiFe(0.7)Mn(0.3)O(3) Ceramics
por: Karpinsky, Dmitry V., et al.
Publicado: (2022)