Evidence for the transition from primary to peritectic phase growth during solidification of undercooled Ni-Zr alloy levitated by electromagnetic field
The Ni(83.25)Zr(16.75) peritectic alloy was undercooled by electromagnetic levitation method up to 198 K. The measured dendritic growth velocity shows a steep acceleration at a critical undercooling of ΔT(crit) = 124 K, which provides an evidence of the transition of the primary growth mode from Ni(...
Autores principales: | Lü, P., Zhou, K., Wang, H. P. |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
Nature Publishing Group
2016
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC5153629/ https://www.ncbi.nlm.nih.gov/pubmed/27958359 http://dx.doi.org/10.1038/srep39042 |
Ejemplares similares
-
On migration of primary/peritectic interface during interrupted directional solidification of Sn-Ni peritectic alloy
por: Peng, Peng, et al.
Publicado: (2016) -
Direct formation of peritectic phase but no primary phase appearance within Ni(83.25)Zr(16.75) peritectic alloy during free fall
por: Lü, P., et al.
Publicado: (2016) -
Simulation of the Peritectic Phase Transition in Fe-C Alloys
por: Fang, Hui, et al.
Publicado: (2022) -
The effect of phosphorus on solidification behaviour of undercooled Al–70 wt.%Si alloys
por: Dang, Bo, et al.
Publicado: (2020) -
The recalescence rate of cooling curve for undercooled solidification
por: Xu, Junfeng, et al.
Publicado: (2020)