Preparation of NASICON-Type Nanosized Solid Electrolyte Li(1.4)Al(0.4)Ti(1.6)(PO(4))(3) by Evaporation-Induced Self-Assembly for Lithium-Ion Battery
A simple and practicable evaporation-induced self-assembly (EISA) method is introduced for the first time to prepare nanosized solid electrolyte Li(1.4)Al(0.4)Ti(1.6)(PO(4))(3) (LATP) for all-solid-state lithium-ion batteries. A pure Na(+) super ion conductor (NASICON) phase is confirmed by X-ray di...
Autores principales: | Liu, Xingang, Fu, Ju, Zhang, Chuhong |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
Springer US
2016
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC5159412/ https://www.ncbi.nlm.nih.gov/pubmed/27981524 http://dx.doi.org/10.1186/s11671-016-1768-z |
Ejemplares similares
-
NASICON-related Na(3.4)Mn(0.4)Fe(1.6)(PO(4))(3)
por: Yatskin, Michael M., et al.
Publicado: (2012) -
Porous NASICON-Type Li(3)Fe(2)(PO(4))(3) Thin Film Deposited by RF Sputtering as Cathode Material for Li-Ion Microbatteries
por: Sugiawati, Vinsensia Ade, et al.
Publicado: (2016) -
In situ Electrochemical-AFM Study of LiFePO(4) Thin Film in Aqueous Electrolyte
por: Wu, Jiaxiong, et al.
Publicado: (2016) -
NASICON-type Na(3)V(2)(PO(4))(3)
por: Zatovsky, Igor V.
Publicado: (2010) -
RbSn(2)(PO(4))(3), a NASICON-type phosphate
por: Zhao, Dan, et al.
Publicado: (2011)