Cargando…

Reduction of arsenic content in a complex galena concentrate by Acidithiobacillus ferrooxidans

BACKGROUND: Bioleaching is a process that has been used in the past in mineral pretreatment of refractory sulfides, mainly in the gold, copper and uranium benefit. This technology has been proved to be cheaper, more efficient and environmentally friendly than roasting and high pressure moisture heat...

Descripción completa

Detalles Bibliográficos
Autores principales: Makita, Mario, Esperón, Margarita, Pereyra, Benito, López, Alejandro, Orrantia, Erasmo
Formato: Texto
Lenguaje:English
Publicado: BioMed Central 2004
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC526773/
https://www.ncbi.nlm.nih.gov/pubmed/15482595
http://dx.doi.org/10.1186/1472-6750-4-22
_version_ 1782121945932759040
author Makita, Mario
Esperón, Margarita
Pereyra, Benito
López, Alejandro
Orrantia, Erasmo
author_facet Makita, Mario
Esperón, Margarita
Pereyra, Benito
López, Alejandro
Orrantia, Erasmo
author_sort Makita, Mario
collection PubMed
description BACKGROUND: Bioleaching is a process that has been used in the past in mineral pretreatment of refractory sulfides, mainly in the gold, copper and uranium benefit. This technology has been proved to be cheaper, more efficient and environmentally friendly than roasting and high pressure moisture heating processes. So far the most studied microorganism in bioleaching is Acidithiobacillus ferrooxidans. There are a few studies about the benefit of metals of low value through bioleaching. From all of these, there are almost no studies dealing with complex minerals containing arsenopyrite (FeAsS). Reduction and/or elimination of arsenic in these ores increase their value and allows the exploitation of a vast variety of minerals that today are being underexploited. RESULTS: Arsenopyrite was totally oxidized. The sum of arsenic remaining in solution and removed by sampling represents from 22 to 33% in weight (yield) of the original content in the mineral. The rest of the biooxidized arsenic form amorphous compounds that precipitate. Galena (PbS) was totally oxidized too, anglesite (PbSO(4)) formed is virtually insoluble and remains in the solids. The influence of seven factors in a batch process was studied. The maximum rate of arsenic dissolution in the concentrate was found using the following levels of factors: small surface area of particle exposure, low pulp density, injecting air and adding 9 K medium to the system. It was also found that ferric chloride and carbon dioxide decreased the arsenic dissolution rate. Bioleaching kinetic data of arsenic solubilization were used to estimate the dilution rate for a continuous culture. Calculated dilution rates were relatively small (0.088–0.103 day(-1)). CONCLUSION: Proper conditions of solubilization of arsenic during bioleaching are key features to improve the percentage (22 to 33% in weight) of arsenic removal. Further studies are needed to determine other factors that influence specifically the solubilization of arsenic in the bioleaching system such as: pH, dissolved oxygen concentration, redox potentials, nature of concentrate and temperature among others. At. ferrooxidans was able to completely oxidize the minerals present during the arsenic bioleaching. Other elements present originally in the concentrate such as Zn, Sb, and Cu were also solubilized. The process of bioleaching is expected to be influenced by mechanisms that still need to be established due to the diversity of the minerals involved and by the presence of traces of metals in the concentrate. The increase in pulp density generates a decrease in the dissolved arsenic concentration. This decrease is greater in runs where air was not injected to the system. The maximum rate of arsenic dissolution in the concentrate was found using; small surface area of particle exposure, low pulp density, injecting air and adding 9 K medium to the system. The effect of addition of ferric chloride during the arsenic bioleaching resulted in a decrease of the solubilized arsenic in the system. The presence of CO(2 )is associated to the decrease in arsenic dissolution.
format Text
id pubmed-526773
institution National Center for Biotechnology Information
language English
publishDate 2004
publisher BioMed Central
record_format MEDLINE/PubMed
spelling pubmed-5267732004-11-12 Reduction of arsenic content in a complex galena concentrate by Acidithiobacillus ferrooxidans Makita, Mario Esperón, Margarita Pereyra, Benito López, Alejandro Orrantia, Erasmo BMC Biotechnol Research Article BACKGROUND: Bioleaching is a process that has been used in the past in mineral pretreatment of refractory sulfides, mainly in the gold, copper and uranium benefit. This technology has been proved to be cheaper, more efficient and environmentally friendly than roasting and high pressure moisture heating processes. So far the most studied microorganism in bioleaching is Acidithiobacillus ferrooxidans. There are a few studies about the benefit of metals of low value through bioleaching. From all of these, there are almost no studies dealing with complex minerals containing arsenopyrite (FeAsS). Reduction and/or elimination of arsenic in these ores increase their value and allows the exploitation of a vast variety of minerals that today are being underexploited. RESULTS: Arsenopyrite was totally oxidized. The sum of arsenic remaining in solution and removed by sampling represents from 22 to 33% in weight (yield) of the original content in the mineral. The rest of the biooxidized arsenic form amorphous compounds that precipitate. Galena (PbS) was totally oxidized too, anglesite (PbSO(4)) formed is virtually insoluble and remains in the solids. The influence of seven factors in a batch process was studied. The maximum rate of arsenic dissolution in the concentrate was found using the following levels of factors: small surface area of particle exposure, low pulp density, injecting air and adding 9 K medium to the system. It was also found that ferric chloride and carbon dioxide decreased the arsenic dissolution rate. Bioleaching kinetic data of arsenic solubilization were used to estimate the dilution rate for a continuous culture. Calculated dilution rates were relatively small (0.088–0.103 day(-1)). CONCLUSION: Proper conditions of solubilization of arsenic during bioleaching are key features to improve the percentage (22 to 33% in weight) of arsenic removal. Further studies are needed to determine other factors that influence specifically the solubilization of arsenic in the bioleaching system such as: pH, dissolved oxygen concentration, redox potentials, nature of concentrate and temperature among others. At. ferrooxidans was able to completely oxidize the minerals present during the arsenic bioleaching. Other elements present originally in the concentrate such as Zn, Sb, and Cu were also solubilized. The process of bioleaching is expected to be influenced by mechanisms that still need to be established due to the diversity of the minerals involved and by the presence of traces of metals in the concentrate. The increase in pulp density generates a decrease in the dissolved arsenic concentration. This decrease is greater in runs where air was not injected to the system. The maximum rate of arsenic dissolution in the concentrate was found using; small surface area of particle exposure, low pulp density, injecting air and adding 9 K medium to the system. The effect of addition of ferric chloride during the arsenic bioleaching resulted in a decrease of the solubilized arsenic in the system. The presence of CO(2 )is associated to the decrease in arsenic dissolution. BioMed Central 2004-10-13 /pmc/articles/PMC526773/ /pubmed/15482595 http://dx.doi.org/10.1186/1472-6750-4-22 Text en Copyright © 2004 Makita et al; licensee BioMed Central Ltd.
spellingShingle Research Article
Makita, Mario
Esperón, Margarita
Pereyra, Benito
López, Alejandro
Orrantia, Erasmo
Reduction of arsenic content in a complex galena concentrate by Acidithiobacillus ferrooxidans
title Reduction of arsenic content in a complex galena concentrate by Acidithiobacillus ferrooxidans
title_full Reduction of arsenic content in a complex galena concentrate by Acidithiobacillus ferrooxidans
title_fullStr Reduction of arsenic content in a complex galena concentrate by Acidithiobacillus ferrooxidans
title_full_unstemmed Reduction of arsenic content in a complex galena concentrate by Acidithiobacillus ferrooxidans
title_short Reduction of arsenic content in a complex galena concentrate by Acidithiobacillus ferrooxidans
title_sort reduction of arsenic content in a complex galena concentrate by acidithiobacillus ferrooxidans
topic Research Article
url https://www.ncbi.nlm.nih.gov/pmc/articles/PMC526773/
https://www.ncbi.nlm.nih.gov/pubmed/15482595
http://dx.doi.org/10.1186/1472-6750-4-22
work_keys_str_mv AT makitamario reductionofarseniccontentinacomplexgalenaconcentratebyacidithiobacillusferrooxidans
AT esperonmargarita reductionofarseniccontentinacomplexgalenaconcentratebyacidithiobacillusferrooxidans
AT pereyrabenito reductionofarseniccontentinacomplexgalenaconcentratebyacidithiobacillusferrooxidans
AT lopezalejandro reductionofarseniccontentinacomplexgalenaconcentratebyacidithiobacillusferrooxidans
AT orrantiaerasmo reductionofarseniccontentinacomplexgalenaconcentratebyacidithiobacillusferrooxidans