Nanooxide/Polymer Composites with Silica@PDMS and Ceria–Zirconia–Silica@PDMS: Textural, Morphological, and Hydrophilic/Hydrophobic Features

SiO(2)@PDMS and CeO(2)–ZrO(2)–SiO(2)@PDMS nanocomposites were prepared and studied using nitrogen adsorption–desorption, Fourier transform infrared spectroscopy (FT-IR), scanning electron microscopy (SEM), measurements of advancing and receding contact angles with water, and microcalorimetry. The po...

Descripción completa

Detalles Bibliográficos
Autores principales: Sulym, Iryna, Goncharuk, Olena, Sternik, Dariusz, Terpilowski, Konrad, Derylo-Marczewska, Anna, Borysenko, Mykola V., Gun’ko, Vladimir M.
Formato: Online Artículo Texto
Lenguaje:English
Publicado: Springer US 2017
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC5328891/
https://www.ncbi.nlm.nih.gov/pubmed/28249372
http://dx.doi.org/10.1186/s11671-017-1935-x
Descripción
Sumario:SiO(2)@PDMS and CeO(2)–ZrO(2)–SiO(2)@PDMS nanocomposites were prepared and studied using nitrogen adsorption–desorption, Fourier transform infrared spectroscopy (FT-IR), scanning electron microscopy (SEM), measurements of advancing and receding contact angles with water, and microcalorimetry. The pore size distributions indicate that the textural characteristics change after oxide modification by poly(dimethylsiloxane) (PDMS). Composites are characterized by mainly mesoporosity and macroporosity of aggregates of oxide nanoparticles or oxide@PDMS nanoparticles and their agglomerates. The FT-IR spectra show that PDMS molecules cover well the oxide surface, since the intensity of the band of free silanols at 3748 cm(−1) decreases with increasing PDMS concentration and it is absent in the IR spectrum at C (PDMS) ≥ 20 wt% that occurs due to the hydrogen bonding of the PDMS molecules to the surface hydroxyls. SEM images reveal that the inter-particle voids are gradually filled and aggregates are re-arranged and increase from 20 to 200 nm in size with the increasing polymer concentration. The highest hydrophobicity (contact angle θ = 140° at C (PDMS) = 20–40 wt%) is obtained for the CeO(2)–ZrO(2)–SiO(2)@PDMS nanocomposites. The heat of composite immersion in water shows a tendency to decrease with increasing PDMS concentration.