Cargando…
Effect of Systematic Control of Pd Thickness and Annealing Temperature on the Fabrication and Evolution of Palladium Nanostructures on Si (111) via the Solid State Dewetting
Si-based optoelectronic devices embedded with metallic nanoparticles (NPs) have demonstrated the NP shape, size, spacing, and crystallinity dependent on light absorption and emission induced by the localized surface plasmon resonance. In this work, we demonstrate various sizes and configurations of...
Autores principales: | , , , , , |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
Springer US
2017
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC5438330/ https://www.ncbi.nlm.nih.gov/pubmed/28532130 http://dx.doi.org/10.1186/s11671-017-2138-1 |
_version_ | 1783237734627803136 |
---|---|
author | Kunwar, Sundar Pandey, Puran Sui, Mao Zhang, Quanzhen Li, Ming-Yu Lee, Jihoon |
author_facet | Kunwar, Sundar Pandey, Puran Sui, Mao Zhang, Quanzhen Li, Ming-Yu Lee, Jihoon |
author_sort | Kunwar, Sundar |
collection | PubMed |
description | Si-based optoelectronic devices embedded with metallic nanoparticles (NPs) have demonstrated the NP shape, size, spacing, and crystallinity dependent on light absorption and emission induced by the localized surface plasmon resonance. In this work, we demonstrate various sizes and configurations of palladium (Pd) nanostructures on Si (111) by the systematic thermal annealing with the variation of Pd thickness and annealing temperature. The evolution of Pd nanostructures are systematically controlled by the dewetting of thin film by means of the surface diffusion in conjunction with the surface and interface energy minimization and Volmer-Weber growth model. Depending on the control of deposition amount ranging between 0.5 and 100 nm at various annealing temperatures, four distinctive regimes of Pd nanostructures are demonstrated: (i) small pits and grain formation, (ii) nucleation and growth of NPs, (iii) lateral evolution of NPs, and (iv) merged nanostructures. In addition, by the control of annealing between 300 and 800 °C, the Pd nanostructures show the evolution of small pits and grains, isolated NPs, and finally, Pd NP-assisted nanohole formation along with the Si decomposition and Pd-Si inter-diffusion. The Raman analysis showed the discrepancies on phonon modes of Si (111) such that the decreased peak intensity with left shift after the fabrication of Pd nanostructures. Furthermore, the UV-VIS-NIR reflectance spectra revealed the existence of surface morphology dependent on absorption, scattering, and reflectance properties. ELECTRONIC SUPPLEMENTARY MATERIAL: The online version of this article (doi:10.1186/s11671-017-2138-1) contains supplementary material, which is available to authorized users. |
format | Online Article Text |
id | pubmed-5438330 |
institution | National Center for Biotechnology Information |
language | English |
publishDate | 2017 |
publisher | Springer US |
record_format | MEDLINE/PubMed |
spelling | pubmed-54383302017-06-06 Effect of Systematic Control of Pd Thickness and Annealing Temperature on the Fabrication and Evolution of Palladium Nanostructures on Si (111) via the Solid State Dewetting Kunwar, Sundar Pandey, Puran Sui, Mao Zhang, Quanzhen Li, Ming-Yu Lee, Jihoon Nanoscale Res Lett Nano Express Si-based optoelectronic devices embedded with metallic nanoparticles (NPs) have demonstrated the NP shape, size, spacing, and crystallinity dependent on light absorption and emission induced by the localized surface plasmon resonance. In this work, we demonstrate various sizes and configurations of palladium (Pd) nanostructures on Si (111) by the systematic thermal annealing with the variation of Pd thickness and annealing temperature. The evolution of Pd nanostructures are systematically controlled by the dewetting of thin film by means of the surface diffusion in conjunction with the surface and interface energy minimization and Volmer-Weber growth model. Depending on the control of deposition amount ranging between 0.5 and 100 nm at various annealing temperatures, four distinctive regimes of Pd nanostructures are demonstrated: (i) small pits and grain formation, (ii) nucleation and growth of NPs, (iii) lateral evolution of NPs, and (iv) merged nanostructures. In addition, by the control of annealing between 300 and 800 °C, the Pd nanostructures show the evolution of small pits and grains, isolated NPs, and finally, Pd NP-assisted nanohole formation along with the Si decomposition and Pd-Si inter-diffusion. The Raman analysis showed the discrepancies on phonon modes of Si (111) such that the decreased peak intensity with left shift after the fabrication of Pd nanostructures. Furthermore, the UV-VIS-NIR reflectance spectra revealed the existence of surface morphology dependent on absorption, scattering, and reflectance properties. ELECTRONIC SUPPLEMENTARY MATERIAL: The online version of this article (doi:10.1186/s11671-017-2138-1) contains supplementary material, which is available to authorized users. Springer US 2017-05-19 /pmc/articles/PMC5438330/ /pubmed/28532130 http://dx.doi.org/10.1186/s11671-017-2138-1 Text en © The Author(s). 2017 Open AccessThis article is distributed under the terms of the Creative Commons Attribution 4.0 International License (http://creativecommons.org/licenses/by/4.0/), which permits unrestricted use, distribution, and reproduction in any medium, provided you give appropriate credit to the original author(s) and the source, provide a link to the Creative Commons license, and indicate if changes were made. |
spellingShingle | Nano Express Kunwar, Sundar Pandey, Puran Sui, Mao Zhang, Quanzhen Li, Ming-Yu Lee, Jihoon Effect of Systematic Control of Pd Thickness and Annealing Temperature on the Fabrication and Evolution of Palladium Nanostructures on Si (111) via the Solid State Dewetting |
title | Effect of Systematic Control of Pd Thickness and Annealing Temperature on the Fabrication and Evolution of Palladium Nanostructures on Si (111) via the Solid State Dewetting |
title_full | Effect of Systematic Control of Pd Thickness and Annealing Temperature on the Fabrication and Evolution of Palladium Nanostructures on Si (111) via the Solid State Dewetting |
title_fullStr | Effect of Systematic Control of Pd Thickness and Annealing Temperature on the Fabrication and Evolution of Palladium Nanostructures on Si (111) via the Solid State Dewetting |
title_full_unstemmed | Effect of Systematic Control of Pd Thickness and Annealing Temperature on the Fabrication and Evolution of Palladium Nanostructures on Si (111) via the Solid State Dewetting |
title_short | Effect of Systematic Control of Pd Thickness and Annealing Temperature on the Fabrication and Evolution of Palladium Nanostructures on Si (111) via the Solid State Dewetting |
title_sort | effect of systematic control of pd thickness and annealing temperature on the fabrication and evolution of palladium nanostructures on si (111) via the solid state dewetting |
topic | Nano Express |
url | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC5438330/ https://www.ncbi.nlm.nih.gov/pubmed/28532130 http://dx.doi.org/10.1186/s11671-017-2138-1 |
work_keys_str_mv | AT kunwarsundar effectofsystematiccontrolofpdthicknessandannealingtemperatureonthefabricationandevolutionofpalladiumnanostructuresonsi111viathesolidstatedewetting AT pandeypuran effectofsystematiccontrolofpdthicknessandannealingtemperatureonthefabricationandevolutionofpalladiumnanostructuresonsi111viathesolidstatedewetting AT suimao effectofsystematiccontrolofpdthicknessandannealingtemperatureonthefabricationandevolutionofpalladiumnanostructuresonsi111viathesolidstatedewetting AT zhangquanzhen effectofsystematiccontrolofpdthicknessandannealingtemperatureonthefabricationandevolutionofpalladiumnanostructuresonsi111viathesolidstatedewetting AT limingyu effectofsystematiccontrolofpdthicknessandannealingtemperatureonthefabricationandevolutionofpalladiumnanostructuresonsi111viathesolidstatedewetting AT leejihoon effectofsystematiccontrolofpdthicknessandannealingtemperatureonthefabricationandevolutionofpalladiumnanostructuresonsi111viathesolidstatedewetting |