Room-temperature Magnetism in Carbon Dots and Enhanced Ferromagnetism in Carbon Dots-Polyaniline Nanocomposite

Room temperature magnetic ordering is reported for very small carbon dots (CDs), mat-like polyaniline nanofibers (Mat-PANI) and a composite of CDs@Mat-PANI containing 0.315 wt% CDs. We have found saturation magnetization (M (S)) of CDs, Mat-PANI and CDs@Mat-PANI at 5 (20/300) K equals to 0.0079 (0.0...

Descripción completa

Detalles Bibliográficos
Autores principales: Liu, Jian, Bi, Hong, Cesar Morais, Paulo, Zhang, Xiang, Zhang, Fapei, Hu, Lin
Formato: Online Artículo Texto
Lenguaje:English
Publicado: Nature Publishing Group UK 2017
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC5438339/
https://www.ncbi.nlm.nih.gov/pubmed/28526848
http://dx.doi.org/10.1038/s41598-017-01350-x
Descripción
Sumario:Room temperature magnetic ordering is reported for very small carbon dots (CDs), mat-like polyaniline nanofibers (Mat-PANI) and a composite of CDs@Mat-PANI containing 0.315 wt% CDs. We have found saturation magnetization (M (S)) of CDs, Mat-PANI and CDs@Mat-PANI at 5 (20/300) K equals to 0.0079 (0.0048/0.0019), 0.0116 (0.0065/0.0055) and 0.0349 (0.0085/0.0077) emu/g, respectively. The M (S) enhancement in CDs@Mat-PANI (200% and 40% at 5 K and 300 K, respectively) is attributed to electron transfer from Mat-PANI imine N-atoms to the encapsulated CDs. Changes in M (S) values reveal that 0.81 (0.08) electron/CD is transferred at 5 (300) K, which is supported by observation of CDs photoluminescence (PL) redshift while in CDs@Mat-PANI. Band-bending and bandgap-renormalization calculations are used to predict a redshift of 117 meV at 300 K as a result of the electron transfer, in excellent agreement with the PL data (110 meV). Raman, X-ray diffraction and X-ray photoelectron spectroscopy data are used to confirm the electron transfer process as well as the strong interaction of CDs with PANI within CDs@Mat-PANI, which increases the crystalline domain size of Mat-PANI from about 4.8 nm to 9.2 nm while reducing the tensile strain from about 6.2% to 1.8%.