Creep Behavior of a Sn-Ag-Bi Pb-Free Solder
Compression creep tests were performed on the ternary 91.84Sn-3.33Ag-4.83Bi (wt.%, abbreviated Sn-Ag-Bi) Pb-free alloy. The test temperatures were: −25 °C, 25 °C, 75 °C, 125 °C, and 160 °C (± 0.5 °C). Four loads were used at the two lowest temperatures and five at the higher temperatures. The specim...
Autores principales: | Vianco, Paul, Rejent, Jerome, Grazier, Mark, Kilgo, Alice |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
MDPI
2012
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC5448995/ http://dx.doi.org/10.3390/ma5112151 |
Ejemplares similares
-
Soldering handbook
por: Vianco, Paul T
Publicado: (1999) -
The Effect of Epoxy Polymer Addition in Sn-Ag-Cu and Sn-Bi Solder Joints
por: Kang, Min-Soo, et al.
Publicado: (2019) -
A Computational Thermodynamics-Assisted Development of Sn-Bi-In-Ga Quaternary Alloys as Low-Temperature Pb-Free Solders
por: Yang, Chih-han, et al.
Publicado: (2019) -
Microstructure and morphology of the soldering interface of Sn–2.0Ag–1.5Zn low Ag content lead-free solder ball and different substrates
por: Xiao, Jin, et al.
Publicado: (2023) -
Interfacial Reaction and Mechanical Properties of Sn-Bi Solder joints
por: Wang, Fengjiang, et al.
Publicado: (2017)