Use of Gypsum as a Preventive Measure for Strength Deterioration during Curing in Class F Fly Ash Geopolymer System
This study discusses strength deterioration during the curing process of fly ash geopolymer and the use of CaSO(4)·2H(2)O (gypsum) as a deterioration remedy when the ash was synthesized using a 10M NaOH and Na-silicate solution. The strength decline was mainly due to the widespread formation of nano...
Autores principales: | Jun, Yubin, Oh, Jae Eun |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
MDPI
2015
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC5455726/ http://dx.doi.org/10.3390/ma8063053 |
Ejemplares similares
-
Benefits of Sealed-Curing on Compressive Strength of Fly Ash-Based Geopolymers
por: Lee, Sujeong, et al.
Publicado: (2016) -
Ambient Cured Fly Ash Geopolymer Coatings for Concrete
por: Biondi, L., et al.
Publicado: (2019) -
Strength and Microstructure of Geopolymer Based on Fly Ash and Metakaolin
por: Barbhuiya, Salim, et al.
Publicado: (2022) -
Performance Optimization and Characterization of Soda Residue-Fly Ash Geopolymer Paste for Goaf Backfill: Beta-Hemihydrate Gypsum Alternative to Sodium Silicate
por: Wang, Haoyu, et al.
Publicado: (2020) -
Study of In Situ Foamed Fly Ash Geopolymer
por: Su, Zijian, et al.
Publicado: (2020)