The Corrosion Behavior of Pure Iron under Solid Na(2)SO(4) Deposit in Wet Oxygen Flow at 500 °C
The corrosion behavior of pure Fe under a Na(2)SO(4) deposit in an atmosphere of O(2) + H(2)O was investigated at 500 °C by thermo gravimetric, and electrochemical measurements, viz. potentiodynamic polarization, electrochemical impedance spectroscopy (EIS), and surface characterization methods viz....
Autores principales: | , , , , |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
MDPI
2014
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC5456147/ https://www.ncbi.nlm.nih.gov/pubmed/28788182 http://dx.doi.org/10.3390/ma7096144 |
_version_ | 1783241183325061120 |
---|---|
author | Tang, Yanbing Liu, Li Fan, Lei Li, Ying Wang, Fuhui |
author_facet | Tang, Yanbing Liu, Li Fan, Lei Li, Ying Wang, Fuhui |
author_sort | Tang, Yanbing |
collection | PubMed |
description | The corrosion behavior of pure Fe under a Na(2)SO(4) deposit in an atmosphere of O(2) + H(2)O was investigated at 500 °C by thermo gravimetric, and electrochemical measurements, viz. potentiodynamic polarization, electrochemical impedance spectroscopy (EIS), and surface characterization methods viz. X-ray diffraction (XRD), and scanning electron microscope (SEM)/energy dispersive spectroscopy(EDS). The results showed that a synergistic effect occurred between Na(2)SO(4) and O(2) + H(2)O, which significantly accelerated the corrosion rate of the pure Fe. Briefly, NaFeO(2) was formed in addition to the customary Fe oxides; at the same time, H(2)SO(4) gas was produced by introduction of water vapor. Subsequently, an electrochemical corrosion reaction occurred due to the existence of Na(2)SO(4), NaFeO(2), and H(2)O. When this coupled to the chemical corrosion reaction, the progress of the chemical corrosion reaction was promoted and eventually resulted in the acceleration of the corrosion of the pure Fe. |
format | Online Article Text |
id | pubmed-5456147 |
institution | National Center for Biotechnology Information |
language | English |
publishDate | 2014 |
publisher | MDPI |
record_format | MEDLINE/PubMed |
spelling | pubmed-54561472017-07-28 The Corrosion Behavior of Pure Iron under Solid Na(2)SO(4) Deposit in Wet Oxygen Flow at 500 °C Tang, Yanbing Liu, Li Fan, Lei Li, Ying Wang, Fuhui Materials (Basel) Article The corrosion behavior of pure Fe under a Na(2)SO(4) deposit in an atmosphere of O(2) + H(2)O was investigated at 500 °C by thermo gravimetric, and electrochemical measurements, viz. potentiodynamic polarization, electrochemical impedance spectroscopy (EIS), and surface characterization methods viz. X-ray diffraction (XRD), and scanning electron microscope (SEM)/energy dispersive spectroscopy(EDS). The results showed that a synergistic effect occurred between Na(2)SO(4) and O(2) + H(2)O, which significantly accelerated the corrosion rate of the pure Fe. Briefly, NaFeO(2) was formed in addition to the customary Fe oxides; at the same time, H(2)SO(4) gas was produced by introduction of water vapor. Subsequently, an electrochemical corrosion reaction occurred due to the existence of Na(2)SO(4), NaFeO(2), and H(2)O. When this coupled to the chemical corrosion reaction, the progress of the chemical corrosion reaction was promoted and eventually resulted in the acceleration of the corrosion of the pure Fe. MDPI 2014-08-27 /pmc/articles/PMC5456147/ /pubmed/28788182 http://dx.doi.org/10.3390/ma7096144 Text en © 2014 by the authors. Licensee MDPI, Basel, Switzerland. This article is an open access article distributed under the terms and conditions of the Creative Commons Attribution license (http://creativecommons.org/licenses/by/3.0/). |
spellingShingle | Article Tang, Yanbing Liu, Li Fan, Lei Li, Ying Wang, Fuhui The Corrosion Behavior of Pure Iron under Solid Na(2)SO(4) Deposit in Wet Oxygen Flow at 500 °C |
title | The Corrosion Behavior of Pure Iron under Solid Na(2)SO(4) Deposit in Wet Oxygen Flow at 500 °C |
title_full | The Corrosion Behavior of Pure Iron under Solid Na(2)SO(4) Deposit in Wet Oxygen Flow at 500 °C |
title_fullStr | The Corrosion Behavior of Pure Iron under Solid Na(2)SO(4) Deposit in Wet Oxygen Flow at 500 °C |
title_full_unstemmed | The Corrosion Behavior of Pure Iron under Solid Na(2)SO(4) Deposit in Wet Oxygen Flow at 500 °C |
title_short | The Corrosion Behavior of Pure Iron under Solid Na(2)SO(4) Deposit in Wet Oxygen Flow at 500 °C |
title_sort | corrosion behavior of pure iron under solid na(2)so(4) deposit in wet oxygen flow at 500 °c |
topic | Article |
url | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC5456147/ https://www.ncbi.nlm.nih.gov/pubmed/28788182 http://dx.doi.org/10.3390/ma7096144 |
work_keys_str_mv | AT tangyanbing thecorrosionbehaviorofpureironundersolidna2so4depositinwetoxygenflowat500c AT liuli thecorrosionbehaviorofpureironundersolidna2so4depositinwetoxygenflowat500c AT fanlei thecorrosionbehaviorofpureironundersolidna2so4depositinwetoxygenflowat500c AT liying thecorrosionbehaviorofpureironundersolidna2so4depositinwetoxygenflowat500c AT wangfuhui thecorrosionbehaviorofpureironundersolidna2so4depositinwetoxygenflowat500c AT tangyanbing corrosionbehaviorofpureironundersolidna2so4depositinwetoxygenflowat500c AT liuli corrosionbehaviorofpureironundersolidna2so4depositinwetoxygenflowat500c AT fanlei corrosionbehaviorofpureironundersolidna2so4depositinwetoxygenflowat500c AT liying corrosionbehaviorofpureironundersolidna2so4depositinwetoxygenflowat500c AT wangfuhui corrosionbehaviorofpureironundersolidna2so4depositinwetoxygenflowat500c |