The Corrosion Behavior of Pure Iron under Solid Na(2)SO(4) Deposit in Wet Oxygen Flow at 500 °C
The corrosion behavior of pure Fe under a Na(2)SO(4) deposit in an atmosphere of O(2) + H(2)O was investigated at 500 °C by thermo gravimetric, and electrochemical measurements, viz. potentiodynamic polarization, electrochemical impedance spectroscopy (EIS), and surface characterization methods viz....
Autores principales: | Tang, Yanbing, Liu, Li, Fan, Lei, Li, Ying, Wang, Fuhui |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
MDPI
2014
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC5456147/ https://www.ncbi.nlm.nih.gov/pubmed/28788182 http://dx.doi.org/10.3390/ma7096144 |
Ejemplares similares
-
Corrosion Behavior of Ti60 Alloy under a Solid NaCl Deposit in Wet Oxygen Flow at 600 °C
por: Fan, Lei, et al.
Publicado: (2016) -
Effects of the Different Solid Deposits on the Corrosion Behavior of Pure Fe in Water Vapor at 500°C
por: Tang, Yanbing, et al.
Publicado: (2020) -
Effects of pre-oxidation on the corrosion behavior of pure Ti under coexistence of solid NaCl deposit and humid oxygen at 600 °C: the diffusion of chlorine
por: Fan, Lei, et al.
Publicado: (2020) -
Corrosion-driven droplet wetting on iron nanolayers
por: Ricard, Aurelien, et al.
Publicado: (2023) -
Effect of Iron Content on Corrosion Properties of Pure Titanium as Grain Refiner
por: Seo, Bosung, et al.
Publicado: (2021)