Cargando…
Effects of Intercritical Annealing Temperature on Mechanical Properties of Fe-7.9Mn-0.14Si-0.05Al-0.07C Steel
A medium Mn steel has been designed to achieve an excellent combination of strength and ductility based on the TRIP (Transformation Induced Plasticity) concept for automotive applications. Following six passes of hot rolling at 850 °C, the Fe-7.9Mn-0.14Si-0.05Al-0.07C (wt.%) steel was warm-rolled at...
Autores principales: | Zhao, Xianming, Shen, Yongfeng, Qiu, Lina, Liu, Yandong, Sun, Xin, Zuo, Liang |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
MDPI
2014
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC5456441/ https://www.ncbi.nlm.nih.gov/pubmed/28788282 http://dx.doi.org/10.3390/ma7127891 |
Ejemplares similares
-
Fe(0.79)Si(0.07)B(0.14) metallic glass gaskets for high-pressure research beyond 1 Mbar
por: Dong, Weiwei, et al.
Publicado: (2022) -
Tuning of the Structure and Magnetocaloric Effect of Mn(1−x)Zr(x)CoGe Alloys (Where x = 0.03, 0.05, 0.07, and 0.1)
por: Kutynia, Karolina, et al.
Publicado: (2021) -
The Effect of Substitution of Mn by Pd on the Structure and Thermomagnetic Properties of the Mn(1−x)Pd(x)CoGe Alloys (Where x = 0.03, 0.05, 0.07 and 0.1)
por: Kutynia, Karolina, et al.
Publicado: (2023) -
Effect of Isothermal Annealing on Sn Whisker Growth Behavior of Sn0.7Cu0.05Ni Solder Joint
por: Hashim, Aimi Noorliyana, et al.
Publicado: (2023) -
Raman scattering and red emission of Mn(4+) in La(0.7)Sr(0.25)Na(0.05)Mn(0.7)Ti(0.3)O(3) manganite phosphor for LED applications
por: Raddaoui, Z., et al.
Publicado: (2020)