Freckle Defect Formation near the Casting Interfaces of Directionally Solidified Superalloys
Freckle defects usually appear on the surface of castings and industrial ingots during the directional solidification process and most of them are located near the interface between the shell mold and superalloys. Ceramic cores create more interfaces in the directionally solidified (DS) and single c...
Autores principales: | Hong, Jianping, Ma, Dexin, Wang, Jun, Wang, Fu, Sun, Baode, Dong, Anping, Li, Fei, Bührig-Polaczek, Andreas |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
MDPI
2016
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC5457264/ https://www.ncbi.nlm.nih.gov/pubmed/28774050 http://dx.doi.org/10.3390/ma9110929 |
Ejemplares similares
-
Grain Selection in a High-Efficiency 2D Grain Selector During Casting of Single-Crystal Superalloys
por: Zhu, Xintao, et al.
Publicado: (2019) -
Investigation of Start Block and Corresponding Influence for Grain Selection during Casting of Single-Crystal Superalloys
por: Zhu, Xintao, et al.
Publicado: (2019) -
Preferred growth orientation and microsegregation behaviors of eutectic in a nickel-based single-crystal superalloy
por: Wang, Fu, et al.
Publicado: (2015) -
Microstructural Investigations of Ni-Based Superalloys by Directional Solidification Quenching Technique
por: Wittenzellner, Tobias, et al.
Publicado: (2020) -
Effects of Withdrawal Rate on the Microstructure of Directionally Solidified GH4720Li Superalloys
por: Qu, Jinglong, et al.
Publicado: (2019)