Shear Bond Strength of Al(2)O(3) Sandblasted Y-TZP Ceramic to the Orthodontic Metal Bracket
As the proportion of adult orthodontic treatment increases, mainly for aesthetic reasons, orthodontic brackets are directly attached to yttria-stabilized tetragonal zirconia polycrystal (Y-TZP) restorations. This, study analyzed the shear bond strength (SBS) between various surface treated Y-TZP and...
Autores principales: | Byeon, Seon Mi, Lee, Min Ho, Bae, Tae Sung |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
MDPI
2017
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC5459165/ https://www.ncbi.nlm.nih.gov/pubmed/28772508 http://dx.doi.org/10.3390/ma10020148 |
Ejemplares similares
-
Shear Bond Strength between Orthodontic Brackets and Monolithic 4Y-TZP: An In Vitro Study
por: Cakir, Emre, et al.
Publicado: (2023) -
The effect of surface treatment and thermocycling on the shear bond strength of orthodontic brackets to the Y-TZP zirconia ceramics: A systematic review
por: AHMED, Tamzid, et al.
Publicado: (2021) -
Improvement in the Tensile Bond Strength between 3Y-TZP Ceramic and Enamel by Surface Treatments
por: Byeon, Seon-Mi, et al.
Publicado: (2016) -
Shear Bond Strength and Bracket Base Morphology of New and Rebonded Orthodontic Ceramic Brackets
por: Urichianu, Mihai, et al.
Publicado: (2022) -
Shear bond strength of ceramic and metallic orthodontic brackets bonded with self-etching primer and conventional bonding adhesives
por: Arash, Valiollah, et al.
Publicado: (2017)