Oxidative chemical vapor deposition of polyaniline thin films
Polyaniline (PANI) is synthesized via oxidative chemical vapor deposition (oCVD) using aniline as monomer and antimony pentachloride as oxidant. Microscopy and spectroscopy indicate that oCVD processing conditions influence the PANI film chemistry, oxidation, and doping level. Fourier transform infr...
Autores principales: | Smolin, Yuriy Y, Soroush, Masoud, Lau, Kenneth K S |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
Beilstein-Institut
2017
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC5480348/ https://www.ncbi.nlm.nih.gov/pubmed/28685127 http://dx.doi.org/10.3762/bjnano.8.128 |
Ejemplares similares
-
Synthesis of coaxial nanotubes of polyaniline and poly(hydroxyethyl methacrylate) by oxidative/initiated chemical vapor deposition
por: Balkan, Alper, et al.
Publicado: (2017) -
Niobium Nitride Thin Films deposited by High Temperature Chemical Vapor Deposition
por: Mercier, F
Publicado: (2014) -
Synthesis of Cobalt Oxides Thin Films Fractal Structures by Laser Chemical Vapor Deposition
por: Haniam, P., et al.
Publicado: (2014) -
Physical vapor deposition of thin films
por: Mahan, John E
Publicado: (2000) -
Chemical vapor deposition polymerization: the growth and properties of parylene thin films
por: Fortin, Jeffrey B, et al.
Publicado: (2004)