Stability of Nanocrystalline Spark Plasma Sintered 3Y-TZP

Spark plasma sintered 3Y-TZP has been investigated with respect to hydrothermal ageing and grinding. The sintering was performed between the temperatures of 1,100 and 1,600 °C for a soaking time of 5 minutes and the resulting materials were obtained with grain sizes between 65 to 800 nm and relative...