Effect of Anatomical Customization of the Fiber Post on the Bond Strength of a Self-Adhesive Resin Cement

AIM: The aim of the study was to evaluate, by means of the push-out test, the effect of the anatomical customization of the fiber post on the bond strength of a self-adhesive resin cement. METHODS: Twelve endodontically treated, human, upper central incisors were randomly divided into two groups (n...

Descripción completa

Detalles Bibliográficos
Autores principales: Rocha, Adricyla Teixeira, Gonçalves, Leticia Machado, Vasconcelos, Ana Júlia de Carvalho, Matos Maia Filho, Etevaldo, Nunes Carvalho, Ceci, De Jesus Tavarez, Rudys Rodolfo
Formato: Online Artículo Texto
Lenguaje:English
Publicado: Hindawi 2017
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC5530420/
https://www.ncbi.nlm.nih.gov/pubmed/28785281
http://dx.doi.org/10.1155/2017/5010712
Descripción
Sumario:AIM: The aim of the study was to evaluate, by means of the push-out test, the effect of the anatomical customization of the fiber post on the bond strength of a self-adhesive resin cement. METHODS: Twelve endodontically treated, human, upper central incisors were randomly divided into two groups (n = 6): control (glass fiber posts cemented with Relyx® U200) and customized (glass fiber posts anatomically customized with translucent composite resin cemented with Relyx U200). The roots were sectioned into three slices, cervical, middle, and apical, and photographed with a digital camera attached to a stereomicroscopic loupe. The images were analyzed by software, for evaluation of the cement line. The slices were subsequently submitted to the push-out test until the post had completely extruded, and the fracture mode was analyzed with a stereomicroscopic loupe. RESULTS: The results showed significant differences between the groups in the different root thirds in relation to the area occupied by air bubbles (p < 0.05). Bond strength, when all the thirds are considered, was 8.77 ± 4.89 MPa for the control group and 16.96 ± 4.85 MPa for the customized group. CONCLUSION: The customized group showed greater bond resistance than the control group and a more uniform cement layer.