Cargando…

Si Wire Supported MnO(2)/Al/Fluorocarbon 3D Core/Shell Nanoenergetic Arrays with Long-Term Storage Stability

Three-dimensional MnO(2)/Al/fluorocarbon core/shell nanoenergetic arrays are prepared on silicon substrate that is with silicon wires on top. Silicon wires are first prepared as the scaffolds by maskless deep reactive ion etching of silicon wafer, which is followed by the hydrothermal growth of MnO(...

Descripción completa

Detalles Bibliográficos
Autores principales: Zhu, Ying, Zhou, Xiang, Wu, Chun, Cheng, Hua, Lu, Zhouguang, Zhang, Kaili
Formato: Online Artículo Texto
Lenguaje:English
Publicado: Nature Publishing Group UK 2017
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC5532262/
https://www.ncbi.nlm.nih.gov/pubmed/28751681
http://dx.doi.org/10.1038/s41598-017-07148-1
Descripción
Sumario:Three-dimensional MnO(2)/Al/fluorocarbon core/shell nanoenergetic arrays are prepared on silicon substrate that is with silicon wires on top. Silicon wires are first prepared as the scaffolds by maskless deep reactive ion etching of silicon wafer, which is followed by the hydrothermal growth of MnO(2). Al and fluorocarbon are then deposited sequentially around the silicon wire (Si-W) supported MnO(2) arrays by magnetron sputtering to realize the core/shell nanoenergetic composite. Several characterization techniques are used to investigate the prepared Si-W/MnO(2)/Al/fluorocarbon arrays, including the scanning electron microscopy, transmission electron microscopy, energy dispersive spectroscopy, X-ray photoelectron spectroscopy, and thermal analysis. 3D upright aligned core/shell structure with an intimate contact between MnO(2) and Al is confirmed from the morphological characterization. Superhydrophobicity is achieved after the fluorocarbon coating. Most importantly, the Si-W/MnO(2)/Al/fluorocarbon nanoenergetic arrays show no decay of energy density after 9 months of storage, indicating potential applications in nanoenergetics-on-a-chip when long-term storage is needed.