Highly Efficient Near Infrared Photothermal Conversion Properties of Reduced Tungsten Oxide/Polyurethane Nanocomposites

In this work, novel WO(3-x)/polyurethane (PU) nanocomposites were prepared by ball milling followed by stirring using a planetary mixer/de-aerator. The effects of phase transformation (WO(3) → WO(2.8) → WO(2.72)) and different weight fractions of tungsten oxide on the optical performance, phototherm...

Descripción completa

Detalles Bibliográficos
Autores principales: Chala, Tolesa Fita, Wu, Chang-Mou, Chou, Min-Hui, Gebeyehu, Molla Bahiru, Cheng, Kuo-Bing
Formato: Online Artículo Texto
Lenguaje:English
Publicado: MDPI 2017
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC5535257/
https://www.ncbi.nlm.nih.gov/pubmed/28737689
http://dx.doi.org/10.3390/nano7070191
Descripción
Sumario:In this work, novel WO(3-x)/polyurethane (PU) nanocomposites were prepared by ball milling followed by stirring using a planetary mixer/de-aerator. The effects of phase transformation (WO(3) → WO(2.8) → WO(2.72)) and different weight fractions of tungsten oxide on the optical performance, photothermal conversion, and thermal properties of the prepared nanocomposites were examined. It was found that the nanocomposites exhibited strong photoabsorption in the entire near-infrared (NIR) region of 780–2500 nm and excellent photothermal conversion properties. This is because the particle size of WO(3-x) was greatly reduced by ball milling and they were well-dispersed in the polyurethane matrix. The higher concentration of oxygen vacancies in WO(3-x) contribute to the efficient absorption of NIR light and its conversion into thermal energy. In particular, WO(2.72)/PU nanocomposites showed strong NIR light absorption of ca. 92%, high photothermal conversion, and better thermal conductivity and absorptivity than other WO(3)/PU nanocomposites. Furthermore, when the nanocomposite with 7 wt % concentration of WO(2.72) nanoparticles was irradiated with infrared light, the temperature of the nanocomposite increased rapidly and stabilized at 120 °C after 5 min. This temperature is 52 °C higher than that achieved by pure PU. These nanocomposites are suitable functional materials for solar collectors, smart coatings, and energy-saving applications.