In vitro study of the fracture resistance of monolithic lithium disilicate, monolithic zirconia, and lithium disilicate pressed on zirconia for three-unit fixed dental prostheses
PURPOSE: The purpose of this study was to determine fracture resistance and failure modes of three-unit fixed dental prostheses (FDPs) made of lithium disilicate pressed on zirconia (LZ), monolithic lithium disilicate (ML), and monolithic zirconia (MZ). MATERIALS AND METHODS: Co-Cr alloy three-unit...
Autores principales: | , , , , |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
The Korean Academy of Prosthodontics
2017
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC5582089/ https://www.ncbi.nlm.nih.gov/pubmed/28874990 http://dx.doi.org/10.4047/jap.2017.9.4.244 |
_version_ | 1783261126571589632 |
---|---|
author | Choi, Jae-Won Kim, So-Yeun Bae, Ji-Hyeon Bae, Eun-Bin Huh, Jung-Bo |
author_facet | Choi, Jae-Won Kim, So-Yeun Bae, Ji-Hyeon Bae, Eun-Bin Huh, Jung-Bo |
author_sort | Choi, Jae-Won |
collection | PubMed |
description | PURPOSE: The purpose of this study was to determine fracture resistance and failure modes of three-unit fixed dental prostheses (FDPs) made of lithium disilicate pressed on zirconia (LZ), monolithic lithium disilicate (ML), and monolithic zirconia (MZ). MATERIALS AND METHODS: Co-Cr alloy three-unit metal FDPs model with maxillary first premolar and first molar abutments was fabricated. Three different FDPs groups, LZ, ML, and MZ, were prepared (n = 5 per group). The three-unit FDPs designs were identical for all specimens and cemented with resin cement on the prepared metal model. The region of pontic in FDPs was given 50,000 times of cyclic preloading at 2 Hz via dental chewing simulator and received a static load until fracture with universal testing machine fixed at 10°. The fracture resistance and mode of failure were recorded. Statistical analyses were performed using the Kruskal-Wallis test and Mann-Whitney U test with Bonferroni's correction (α=0.05/3=0.017). RESULTS: A significant difference in fracture resistance was found between LZ (4943.87 ± 1243.70 N) and ML (2872.61 ± 658.78 N) groups, as well as between ML and MZ (4948.02 ± 974.51 N) groups (P<.05), but no significant difference was found between LZ and MZ groups (P>.05). With regard to fracture pattern, there were three cases of veneer chipping and two interfacial fractures in LZ group, and complete fracture was observed in all the specimens of ML and MZ groups. CONCLUSION: Compared to monolithic lithium disilicate FDPs, monolithic zirconia FDPs and lithium disilicate glass ceramics pressed on zirconia-based FDPs showed superior fracture resistance while they manifested comparable fracture resistances. |
format | Online Article Text |
id | pubmed-5582089 |
institution | National Center for Biotechnology Information |
language | English |
publishDate | 2017 |
publisher | The Korean Academy of Prosthodontics |
record_format | MEDLINE/PubMed |
spelling | pubmed-55820892017-09-05 In vitro study of the fracture resistance of monolithic lithium disilicate, monolithic zirconia, and lithium disilicate pressed on zirconia for three-unit fixed dental prostheses Choi, Jae-Won Kim, So-Yeun Bae, Ji-Hyeon Bae, Eun-Bin Huh, Jung-Bo J Adv Prosthodont Original Article PURPOSE: The purpose of this study was to determine fracture resistance and failure modes of three-unit fixed dental prostheses (FDPs) made of lithium disilicate pressed on zirconia (LZ), monolithic lithium disilicate (ML), and monolithic zirconia (MZ). MATERIALS AND METHODS: Co-Cr alloy three-unit metal FDPs model with maxillary first premolar and first molar abutments was fabricated. Three different FDPs groups, LZ, ML, and MZ, were prepared (n = 5 per group). The three-unit FDPs designs were identical for all specimens and cemented with resin cement on the prepared metal model. The region of pontic in FDPs was given 50,000 times of cyclic preloading at 2 Hz via dental chewing simulator and received a static load until fracture with universal testing machine fixed at 10°. The fracture resistance and mode of failure were recorded. Statistical analyses were performed using the Kruskal-Wallis test and Mann-Whitney U test with Bonferroni's correction (α=0.05/3=0.017). RESULTS: A significant difference in fracture resistance was found between LZ (4943.87 ± 1243.70 N) and ML (2872.61 ± 658.78 N) groups, as well as between ML and MZ (4948.02 ± 974.51 N) groups (P<.05), but no significant difference was found between LZ and MZ groups (P>.05). With regard to fracture pattern, there were three cases of veneer chipping and two interfacial fractures in LZ group, and complete fracture was observed in all the specimens of ML and MZ groups. CONCLUSION: Compared to monolithic lithium disilicate FDPs, monolithic zirconia FDPs and lithium disilicate glass ceramics pressed on zirconia-based FDPs showed superior fracture resistance while they manifested comparable fracture resistances. The Korean Academy of Prosthodontics 2017-08 2017-08-16 /pmc/articles/PMC5582089/ /pubmed/28874990 http://dx.doi.org/10.4047/jap.2017.9.4.244 Text en © 2017 The Korean Academy of Prosthodontics http://creativecommons.org/licenses/by-nc/3.0/ This is an Open Access article distributed under the terms of the Creative Commons Attribution Non-Commercial License (http://creativecommons.org/licenses/by-nc/3.0) which permits unrestricted non-commercial use, distribution, and reproduction in any medium, provided the original work is properly cited. |
spellingShingle | Original Article Choi, Jae-Won Kim, So-Yeun Bae, Ji-Hyeon Bae, Eun-Bin Huh, Jung-Bo In vitro study of the fracture resistance of monolithic lithium disilicate, monolithic zirconia, and lithium disilicate pressed on zirconia for three-unit fixed dental prostheses |
title | In vitro study of the fracture resistance of monolithic lithium disilicate, monolithic zirconia, and lithium disilicate pressed on zirconia for three-unit fixed dental prostheses |
title_full | In vitro study of the fracture resistance of monolithic lithium disilicate, monolithic zirconia, and lithium disilicate pressed on zirconia for three-unit fixed dental prostheses |
title_fullStr | In vitro study of the fracture resistance of monolithic lithium disilicate, monolithic zirconia, and lithium disilicate pressed on zirconia for three-unit fixed dental prostheses |
title_full_unstemmed | In vitro study of the fracture resistance of monolithic lithium disilicate, monolithic zirconia, and lithium disilicate pressed on zirconia for three-unit fixed dental prostheses |
title_short | In vitro study of the fracture resistance of monolithic lithium disilicate, monolithic zirconia, and lithium disilicate pressed on zirconia for three-unit fixed dental prostheses |
title_sort | in vitro study of the fracture resistance of monolithic lithium disilicate, monolithic zirconia, and lithium disilicate pressed on zirconia for three-unit fixed dental prostheses |
topic | Original Article |
url | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC5582089/ https://www.ncbi.nlm.nih.gov/pubmed/28874990 http://dx.doi.org/10.4047/jap.2017.9.4.244 |
work_keys_str_mv | AT choijaewon invitrostudyofthefractureresistanceofmonolithiclithiumdisilicatemonolithiczirconiaandlithiumdisilicatepressedonzirconiaforthreeunitfixeddentalprostheses AT kimsoyeun invitrostudyofthefractureresistanceofmonolithiclithiumdisilicatemonolithiczirconiaandlithiumdisilicatepressedonzirconiaforthreeunitfixeddentalprostheses AT baejihyeon invitrostudyofthefractureresistanceofmonolithiclithiumdisilicatemonolithiczirconiaandlithiumdisilicatepressedonzirconiaforthreeunitfixeddentalprostheses AT baeeunbin invitrostudyofthefractureresistanceofmonolithiclithiumdisilicatemonolithiczirconiaandlithiumdisilicatepressedonzirconiaforthreeunitfixeddentalprostheses AT huhjungbo invitrostudyofthefractureresistanceofmonolithiclithiumdisilicatemonolithiczirconiaandlithiumdisilicatepressedonzirconiaforthreeunitfixeddentalprostheses |