Electrospun Gelatin/poly(Glycerol Sebacate) Membrane with Controlled Release of Antibiotics for Wound Dressing

BACKGROUND: The most important risk that threatens the skin wounds is infections. Therefore, fabrication of a membrane as a wound dressing with the ability of antibiotic delivery in a proper delivery rate is especially important. MATERIALS AND METHODS: Poly(glycerol sebacate) (PGS) was prepared from...

Descripción completa

Detalles Bibliográficos
Autores principales: Shirazaki, Parisa, Varshosaz, Jaleh, Kharazi, Anoushe Zargar
Formato: Online Artículo Texto
Lenguaje:English
Publicado: Medknow Publications & Media Pvt Ltd 2017
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC5590405/
https://www.ncbi.nlm.nih.gov/pubmed/28904933
http://dx.doi.org/10.4103/abr.abr_197_16
_version_ 1783262531401285632
author Shirazaki, Parisa
Varshosaz, Jaleh
Kharazi, Anoushe Zargar
author_facet Shirazaki, Parisa
Varshosaz, Jaleh
Kharazi, Anoushe Zargar
author_sort Shirazaki, Parisa
collection PubMed
description BACKGROUND: The most important risk that threatens the skin wounds is infections. Therefore, fabrication of a membrane as a wound dressing with the ability of antibiotic delivery in a proper delivery rate is especially important. MATERIALS AND METHODS: Poly(glycerol sebacate) (PGS) was prepared from sebacic acid and glycerol with 1:1 ratio; then, it was added to gelatin in the 1:3 ratio and was dissolved in 80% (v/v) acetic acid, and finally, ciprofloxacin was added in 10% (w/v) of polymer solution. The gelatin/PGS membrane was fabricated using an electrospinning method. The membrane was cross-linked using ethyl-3-(3-dimethylaminopropyl) carbodiimide ethyl-3-(3-dimethylaminopropyl)carbodiim (EDC) and N-hydroxysuccinimide (NHS) in different time periods to achieve a proper drug release rate. Fourier-transform infrared (FTIR) spectroscopy was being used to manifest the peaks of polymers and drug in the membrane. Scanning electron microscopy (SEM) was used to evaluate the morphology, fibers diameter, pore size, and porosity before and after crosslinking process. Ultraviolet (UV)-visible spectrophotometry was used to show the ciprofloxacin release from the cross-linked membrane. RESULTS: FTIR analysis showed the characteristic peaks of gelatin, PGS, and ciprofloxacin without any added peaks after the crosslinking process. SEM images revealed that nanofibers’ size increased during the crosslinking process and porosity was higher than 80% before and after crosslinking process. UV-visible spectrophotometry showed the proper rate of ciprofloxacin release occurred from cross-linked membrane that remaining in EDC/NHS ethanol solution for 120 min. CONCLUSION: The obtained results suggest that this recently developed gelatin/PGS membrane with controlled release of ciprofloxacin could be a promising biodegradable membrane for wound dressing.
format Online
Article
Text
id pubmed-5590405
institution National Center for Biotechnology Information
language English
publishDate 2017
publisher Medknow Publications & Media Pvt Ltd
record_format MEDLINE/PubMed
spelling pubmed-55904052017-09-13 Electrospun Gelatin/poly(Glycerol Sebacate) Membrane with Controlled Release of Antibiotics for Wound Dressing Shirazaki, Parisa Varshosaz, Jaleh Kharazi, Anoushe Zargar Adv Biomed Res Original Article BACKGROUND: The most important risk that threatens the skin wounds is infections. Therefore, fabrication of a membrane as a wound dressing with the ability of antibiotic delivery in a proper delivery rate is especially important. MATERIALS AND METHODS: Poly(glycerol sebacate) (PGS) was prepared from sebacic acid and glycerol with 1:1 ratio; then, it was added to gelatin in the 1:3 ratio and was dissolved in 80% (v/v) acetic acid, and finally, ciprofloxacin was added in 10% (w/v) of polymer solution. The gelatin/PGS membrane was fabricated using an electrospinning method. The membrane was cross-linked using ethyl-3-(3-dimethylaminopropyl) carbodiimide ethyl-3-(3-dimethylaminopropyl)carbodiim (EDC) and N-hydroxysuccinimide (NHS) in different time periods to achieve a proper drug release rate. Fourier-transform infrared (FTIR) spectroscopy was being used to manifest the peaks of polymers and drug in the membrane. Scanning electron microscopy (SEM) was used to evaluate the morphology, fibers diameter, pore size, and porosity before and after crosslinking process. Ultraviolet (UV)-visible spectrophotometry was used to show the ciprofloxacin release from the cross-linked membrane. RESULTS: FTIR analysis showed the characteristic peaks of gelatin, PGS, and ciprofloxacin without any added peaks after the crosslinking process. SEM images revealed that nanofibers’ size increased during the crosslinking process and porosity was higher than 80% before and after crosslinking process. UV-visible spectrophotometry showed the proper rate of ciprofloxacin release occurred from cross-linked membrane that remaining in EDC/NHS ethanol solution for 120 min. CONCLUSION: The obtained results suggest that this recently developed gelatin/PGS membrane with controlled release of ciprofloxacin could be a promising biodegradable membrane for wound dressing. Medknow Publications & Media Pvt Ltd 2017-08-28 /pmc/articles/PMC5590405/ /pubmed/28904933 http://dx.doi.org/10.4103/abr.abr_197_16 Text en Copyright: © 2017 Advanced Biomedical Research http://creativecommons.org/licenses/by-nc-sa/3.0 This is an open access article distributed under the terms of the Creative Commons Attribution-NonCommercial-ShareAlike 3.0 License, which allows others to remix, tweak, and build upon the work non-commercially, as long as the author is credited and the new creations are licensed under the identical terms.
spellingShingle Original Article
Shirazaki, Parisa
Varshosaz, Jaleh
Kharazi, Anoushe Zargar
Electrospun Gelatin/poly(Glycerol Sebacate) Membrane with Controlled Release of Antibiotics for Wound Dressing
title Electrospun Gelatin/poly(Glycerol Sebacate) Membrane with Controlled Release of Antibiotics for Wound Dressing
title_full Electrospun Gelatin/poly(Glycerol Sebacate) Membrane with Controlled Release of Antibiotics for Wound Dressing
title_fullStr Electrospun Gelatin/poly(Glycerol Sebacate) Membrane with Controlled Release of Antibiotics for Wound Dressing
title_full_unstemmed Electrospun Gelatin/poly(Glycerol Sebacate) Membrane with Controlled Release of Antibiotics for Wound Dressing
title_short Electrospun Gelatin/poly(Glycerol Sebacate) Membrane with Controlled Release of Antibiotics for Wound Dressing
title_sort electrospun gelatin/poly(glycerol sebacate) membrane with controlled release of antibiotics for wound dressing
topic Original Article
url https://www.ncbi.nlm.nih.gov/pmc/articles/PMC5590405/
https://www.ncbi.nlm.nih.gov/pubmed/28904933
http://dx.doi.org/10.4103/abr.abr_197_16
work_keys_str_mv AT shirazakiparisa electrospungelatinpolyglycerolsebacatemembranewithcontrolledreleaseofantibioticsforwounddressing
AT varshosazjaleh electrospungelatinpolyglycerolsebacatemembranewithcontrolledreleaseofantibioticsforwounddressing
AT kharazianoushezargar electrospungelatinpolyglycerolsebacatemembranewithcontrolledreleaseofantibioticsforwounddressing