Fracture Toughness of Nanohybrid and Hybrid Composites Stored Wet and Dry up to 60 Days
STATEMENT OF PROBLEM: Patients’ demand for tooth-colored restoratives in the posterior region is increasing. Clinicians use universal nanohybrid resin composites for both anterior and posterior regions. There are few published reports comparing fracture toughness of nonohybrids and that of hybrid co...
Autores principales: | Sookhakiyan, M., Tavana, S., Azarnia, Y., Bagheri, R. |
---|---|
Formato: | Online Artículo Texto |
Lenguaje: | English |
Publicado: |
Journal of Dental Biomaterials
2017
|
Materias: | |
Acceso en línea: | https://www.ncbi.nlm.nih.gov/pmc/articles/PMC5608048/ https://www.ncbi.nlm.nih.gov/pubmed/28959763 |
Ejemplares similares
-
Physical and Mechanical Properties of Bulk-Fill, Conventional, and Flowable Resin Composites Stored Dry and Wet
por: Jafarpour, Dana, et al.
Publicado: (2022) -
Evaluation of Mode II Fracture Toughness of Hybrid Fibrous Geopolymer Composites
por: Abid, Sallal R., et al.
Publicado: (2021) -
Symposium on Fracture Toughness
por: American Society for Testing and Materials. Philadelphia
Publicado: (1973) -
Effect of the Drying Method of Pine and Beech Wood on Fracture Toughness and Shear Yield Stress
por: Chuchala, Daniel, et al.
Publicado: (2020) -
Photonics and fracture toughness of heterogeneous composite materials
por: Antony, S. Joseph, et al.
Publicado: (2017)