Electrochemical Behaviour and Galvanic Effects of Titanium Implants Coupled to Metallic Suprastructures in Artificial Saliva

The aim of the present study is to analyze the electrochemical behavior of five different dental alloys: two cobalt-chromium alloys (CoCr and CoCr-c), one nickel-chromium-titanium alloy (NiCrTi), one gold-palladium alloy (Au), and one titanium alloy (Ti6Al4V), and the galvanic effect when they are c...

Descripción completa

Detalles Bibliográficos
Autores principales: Mellado-Valero, Ana, Igual Muñoz, Anna, Guiñón Pina, Virginia, Sola-Ruiz, Ma Fernanda
Formato: Online Artículo Texto
Lenguaje:English
Publicado: MDPI 2018
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC5793669/
https://www.ncbi.nlm.nih.gov/pubmed/29361767
http://dx.doi.org/10.3390/ma11010171
_version_ 1783297005864353792
author Mellado-Valero, Ana
Igual Muñoz, Anna
Guiñón Pina, Virginia
Sola-Ruiz, Ma Fernanda
author_facet Mellado-Valero, Ana
Igual Muñoz, Anna
Guiñón Pina, Virginia
Sola-Ruiz, Ma Fernanda
author_sort Mellado-Valero, Ana
collection PubMed
description The aim of the present study is to analyze the electrochemical behavior of five different dental alloys: two cobalt-chromium alloys (CoCr and CoCr-c), one nickel-chromium-titanium alloy (NiCrTi), one gold-palladium alloy (Au), and one titanium alloy (Ti6Al4V), and the galvanic effect when they are coupled to titanium implants (TiG2). It was carried out by electrochemical techniques (open circuit measurements, potentiodynamic curves and Zero-Resistance Ammetry) in artificial saliva (AS), with and without fluorides in different acidic conditions. The studied alloys are spontaneously passivated, but NiCrTi alloy has a very narrow passive domain and losses its passivity in presence of fluorides, so is not considered as a good option for implant superstructures. Variations of pH from 6.5 to 3 in artificial saliva do not change the electrochemical behavior of Ti, Ti6Al4V, and CoCr alloys, and couples, but when the pH of the artificial saliva is below 3.5 and the fluoride content is 1000 ppm Ti and Ti6Al4V starts actively dissolving, and CoCr-c superstructures coupled to Ti show acceleration of corrosion due to galvanic effects. Thus, NiCrTi is not recommended for implant superstructures because of risk of Ni ion release to the body, and fluorides should be avoided in acidic media because Ti, Ti6Al4V, and CoCr-c superstructures show galvanic corrosion. The best combinations are Ti/Ti6Al4V and Ti/CoCr as alternative of noble gold alloys.
format Online
Article
Text
id pubmed-5793669
institution National Center for Biotechnology Information
language English
publishDate 2018
publisher MDPI
record_format MEDLINE/PubMed
spelling pubmed-57936692018-02-07 Electrochemical Behaviour and Galvanic Effects of Titanium Implants Coupled to Metallic Suprastructures in Artificial Saliva Mellado-Valero, Ana Igual Muñoz, Anna Guiñón Pina, Virginia Sola-Ruiz, Ma Fernanda Materials (Basel) Article The aim of the present study is to analyze the electrochemical behavior of five different dental alloys: two cobalt-chromium alloys (CoCr and CoCr-c), one nickel-chromium-titanium alloy (NiCrTi), one gold-palladium alloy (Au), and one titanium alloy (Ti6Al4V), and the galvanic effect when they are coupled to titanium implants (TiG2). It was carried out by electrochemical techniques (open circuit measurements, potentiodynamic curves and Zero-Resistance Ammetry) in artificial saliva (AS), with and without fluorides in different acidic conditions. The studied alloys are spontaneously passivated, but NiCrTi alloy has a very narrow passive domain and losses its passivity in presence of fluorides, so is not considered as a good option for implant superstructures. Variations of pH from 6.5 to 3 in artificial saliva do not change the electrochemical behavior of Ti, Ti6Al4V, and CoCr alloys, and couples, but when the pH of the artificial saliva is below 3.5 and the fluoride content is 1000 ppm Ti and Ti6Al4V starts actively dissolving, and CoCr-c superstructures coupled to Ti show acceleration of corrosion due to galvanic effects. Thus, NiCrTi is not recommended for implant superstructures because of risk of Ni ion release to the body, and fluorides should be avoided in acidic media because Ti, Ti6Al4V, and CoCr-c superstructures show galvanic corrosion. The best combinations are Ti/Ti6Al4V and Ti/CoCr as alternative of noble gold alloys. MDPI 2018-01-22 /pmc/articles/PMC5793669/ /pubmed/29361767 http://dx.doi.org/10.3390/ma11010171 Text en © 2018 by the authors. Licensee MDPI, Basel, Switzerland. This article is an open access article distributed under the terms and conditions of the Creative Commons Attribution (CC BY) license (http://creativecommons.org/licenses/by/4.0/).
spellingShingle Article
Mellado-Valero, Ana
Igual Muñoz, Anna
Guiñón Pina, Virginia
Sola-Ruiz, Ma Fernanda
Electrochemical Behaviour and Galvanic Effects of Titanium Implants Coupled to Metallic Suprastructures in Artificial Saliva
title Electrochemical Behaviour and Galvanic Effects of Titanium Implants Coupled to Metallic Suprastructures in Artificial Saliva
title_full Electrochemical Behaviour and Galvanic Effects of Titanium Implants Coupled to Metallic Suprastructures in Artificial Saliva
title_fullStr Electrochemical Behaviour and Galvanic Effects of Titanium Implants Coupled to Metallic Suprastructures in Artificial Saliva
title_full_unstemmed Electrochemical Behaviour and Galvanic Effects of Titanium Implants Coupled to Metallic Suprastructures in Artificial Saliva
title_short Electrochemical Behaviour and Galvanic Effects of Titanium Implants Coupled to Metallic Suprastructures in Artificial Saliva
title_sort electrochemical behaviour and galvanic effects of titanium implants coupled to metallic suprastructures in artificial saliva
topic Article
url https://www.ncbi.nlm.nih.gov/pmc/articles/PMC5793669/
https://www.ncbi.nlm.nih.gov/pubmed/29361767
http://dx.doi.org/10.3390/ma11010171
work_keys_str_mv AT melladovaleroana electrochemicalbehaviourandgalvaniceffectsoftitaniumimplantscoupledtometallicsuprastructuresinartificialsaliva
AT igualmunozanna electrochemicalbehaviourandgalvaniceffectsoftitaniumimplantscoupledtometallicsuprastructuresinartificialsaliva
AT guinonpinavirginia electrochemicalbehaviourandgalvaniceffectsoftitaniumimplantscoupledtometallicsuprastructuresinartificialsaliva
AT solaruizmafernanda electrochemicalbehaviourandgalvaniceffectsoftitaniumimplantscoupledtometallicsuprastructuresinartificialsaliva