Surface Detail Reproduction and Dimensional Stability of Contemporary Irreversible Hydrocolloid Alternatives after Immediate and Delayed Pouring

PURPOSE: To overcome the poor dimensional stability of irreversible hydrocolloids, alternative materials were introduced. The dimensional changes of these alternatives after delayed pouring are not well studied and documented in the literature. The purpose of the study is to evaluate and compare the...

Descripción completa

Detalles Bibliográficos
Autores principales: Kusugal, Preethi, Chourasiya, Ritu Sunil, Ruttonji, Zarir, Astagi, Preeti, Nayak, Ajay Kumar, Patil, Abhishekha
Formato: Online Artículo Texto
Lenguaje:English
Publicado: Medknow Publications & Media Pvt Ltd 2018
Materias:
Acceso en línea:https://www.ncbi.nlm.nih.gov/pmc/articles/PMC5863403/
https://www.ncbi.nlm.nih.gov/pubmed/29599578
http://dx.doi.org/10.4103/ccd.ccd_676_17
_version_ 1783308381519347712
author Kusugal, Preethi
Chourasiya, Ritu Sunil
Ruttonji, Zarir
Astagi, Preeti
Nayak, Ajay Kumar
Patil, Abhishekha
author_facet Kusugal, Preethi
Chourasiya, Ritu Sunil
Ruttonji, Zarir
Astagi, Preeti
Nayak, Ajay Kumar
Patil, Abhishekha
author_sort Kusugal, Preethi
collection PubMed
description PURPOSE: To overcome the poor dimensional stability of irreversible hydrocolloids, alternative materials were introduced. The dimensional changes of these alternatives after delayed pouring are not well studied and documented in the literature. The purpose of the study is to evaluate and compare the surface detail reproduction and dimensional stability of two irreversible hydrocolloid alternatives with an extended-pour irreversible hydrocolloid at different time intervals. MATERIALS AND METHODS: All testing were performed according to the ANSI/ADA specification number 18 for surface detail reproduction and specification number 19 for dimensional change. The test materials used in this study were newer irreversible hydrocolloid alternatives such as AlgiNot FS, Algin-X Ultra FS, and Kromopan 100 which is an extended pour irreversible hydrocolloid as control. The surface detail reproduction was evaluated using stereomicroscope. The dimensional change after storage period of 1 h, 24 h, and 120 h was assessed and compared between the test materials and control. The data were analyzed using one-way ANOVA and post hoc Bonferroni test. RESULTS: Statistically significant results (P < 0.001) were seen when mean scores of the tested materials were compared with respect to reproduction of 22 μm line from the metal block. Kromopan 100 showed statistically significant differences between different time intervals (P < 0.001) and exhibited more dimensional change. Algin-X Ultra FS proved to be more accurate and dimensionally stable. CONCLUSIONS: Newer irreversible hydrocolloid alternative impression materials were more accurate in surface detail reproduction and exhibited minimal dimensional change after storage period of 1 h, 24 h, and 120 h than extended-pour irreversible hydrocolloid impression material.
format Online
Article
Text
id pubmed-5863403
institution National Center for Biotechnology Information
language English
publishDate 2018
publisher Medknow Publications & Media Pvt Ltd
record_format MEDLINE/PubMed
spelling pubmed-58634032018-03-29 Surface Detail Reproduction and Dimensional Stability of Contemporary Irreversible Hydrocolloid Alternatives after Immediate and Delayed Pouring Kusugal, Preethi Chourasiya, Ritu Sunil Ruttonji, Zarir Astagi, Preeti Nayak, Ajay Kumar Patil, Abhishekha Contemp Clin Dent Original Article PURPOSE: To overcome the poor dimensional stability of irreversible hydrocolloids, alternative materials were introduced. The dimensional changes of these alternatives after delayed pouring are not well studied and documented in the literature. The purpose of the study is to evaluate and compare the surface detail reproduction and dimensional stability of two irreversible hydrocolloid alternatives with an extended-pour irreversible hydrocolloid at different time intervals. MATERIALS AND METHODS: All testing were performed according to the ANSI/ADA specification number 18 for surface detail reproduction and specification number 19 for dimensional change. The test materials used in this study were newer irreversible hydrocolloid alternatives such as AlgiNot FS, Algin-X Ultra FS, and Kromopan 100 which is an extended pour irreversible hydrocolloid as control. The surface detail reproduction was evaluated using stereomicroscope. The dimensional change after storage period of 1 h, 24 h, and 120 h was assessed and compared between the test materials and control. The data were analyzed using one-way ANOVA and post hoc Bonferroni test. RESULTS: Statistically significant results (P < 0.001) were seen when mean scores of the tested materials were compared with respect to reproduction of 22 μm line from the metal block. Kromopan 100 showed statistically significant differences between different time intervals (P < 0.001) and exhibited more dimensional change. Algin-X Ultra FS proved to be more accurate and dimensionally stable. CONCLUSIONS: Newer irreversible hydrocolloid alternative impression materials were more accurate in surface detail reproduction and exhibited minimal dimensional change after storage period of 1 h, 24 h, and 120 h than extended-pour irreversible hydrocolloid impression material. Medknow Publications & Media Pvt Ltd 2018 /pmc/articles/PMC5863403/ /pubmed/29599578 http://dx.doi.org/10.4103/ccd.ccd_676_17 Text en Copyright: © 2018 Contemporary Clinical Dentistry http://creativecommons.org/licenses/by-nc-sa/3.0 This is an open access article distributed under the terms of the Creative Commons Attribution-NonCommercial-ShareAlike 3.0 License, which allows others to remix, tweak, and build upon the work non-commercially, as long as the author is credited and the new creations are licensed under the identical terms.
spellingShingle Original Article
Kusugal, Preethi
Chourasiya, Ritu Sunil
Ruttonji, Zarir
Astagi, Preeti
Nayak, Ajay Kumar
Patil, Abhishekha
Surface Detail Reproduction and Dimensional Stability of Contemporary Irreversible Hydrocolloid Alternatives after Immediate and Delayed Pouring
title Surface Detail Reproduction and Dimensional Stability of Contemporary Irreversible Hydrocolloid Alternatives after Immediate and Delayed Pouring
title_full Surface Detail Reproduction and Dimensional Stability of Contemporary Irreversible Hydrocolloid Alternatives after Immediate and Delayed Pouring
title_fullStr Surface Detail Reproduction and Dimensional Stability of Contemporary Irreversible Hydrocolloid Alternatives after Immediate and Delayed Pouring
title_full_unstemmed Surface Detail Reproduction and Dimensional Stability of Contemporary Irreversible Hydrocolloid Alternatives after Immediate and Delayed Pouring
title_short Surface Detail Reproduction and Dimensional Stability of Contemporary Irreversible Hydrocolloid Alternatives after Immediate and Delayed Pouring
title_sort surface detail reproduction and dimensional stability of contemporary irreversible hydrocolloid alternatives after immediate and delayed pouring
topic Original Article
url https://www.ncbi.nlm.nih.gov/pmc/articles/PMC5863403/
https://www.ncbi.nlm.nih.gov/pubmed/29599578
http://dx.doi.org/10.4103/ccd.ccd_676_17
work_keys_str_mv AT kusugalpreethi surfacedetailreproductionanddimensionalstabilityofcontemporaryirreversiblehydrocolloidalternativesafterimmediateanddelayedpouring
AT chourasiyaritusunil surfacedetailreproductionanddimensionalstabilityofcontemporaryirreversiblehydrocolloidalternativesafterimmediateanddelayedpouring
AT ruttonjizarir surfacedetailreproductionanddimensionalstabilityofcontemporaryirreversiblehydrocolloidalternativesafterimmediateanddelayedpouring
AT astagipreeti surfacedetailreproductionanddimensionalstabilityofcontemporaryirreversiblehydrocolloidalternativesafterimmediateanddelayedpouring
AT nayakajaykumar surfacedetailreproductionanddimensionalstabilityofcontemporaryirreversiblehydrocolloidalternativesafterimmediateanddelayedpouring
AT patilabhishekha surfacedetailreproductionanddimensionalstabilityofcontemporaryirreversiblehydrocolloidalternativesafterimmediateanddelayedpouring